MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Hostalen CRP 100 BLACK (XL) High Density Polyethylene (HDPE), Pipe Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: Hostalen CRP 100 black (XL) is a high density polyethylene (HDPE), black colored similar RAL 9004 with high melt viscosity particularly higher zero viscosity than standard compounds. Typical application: Extrusion of extra large and thick walled pipes to avoid the sagging of the melt and to maintain uniform wall thickness. The product is classified as PE 100 and provides good stress crack resistance properties (ESCR) combined with very good long term hydrostatic strength. Applications: Drinking Water Pipe, Gas Pipe, Industrial, Soil & Waste Pipe

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.959 g/ccISO 1183-1
Oxidative Induction Time (OIT) 30 minISO 11357-6
Carbon Black Loading 2.25 %ISO 6964
Melt Flow 0.23 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133-1
 6.4 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 63
@Time 3.00 sec
ISO 868
Tensile Strength, Yield 23.0 MPa50mm/min; ISO 527-1,-2
Elongation at Break >= 350 %ISO 527-1,-2
Elongation at Yield 8.0 %50mm/min; ISO 527-1,-2
Tensile Modulus 1100 MPaISO 527-1,-2
Flexural Modulus 330 MPacreep, 4 point loading/ 2000 hr; DIN 16841
 560 MPacreep, 4 point loading/ 24 hr; DIN 16841
 1200 MPacreep, 4 point loading/1 min; DIN 16841
Charpy Impact, Notched 13.0 kJ/m²
@Temperature -30.0 °C
ISO 179-1/1eA
 26.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1/1eA
Tensile Creep Modulus, 1 hour 850 MPa
@Pressure 2.00 MPa
ISO 899-1
Tensile Creep Modulus, 1000 hours 360 MPa
@Pressure 2.00 MPa
ISO 899-1
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 74.0 °CB50; ISO 306
DSC Induction Temperature 129 °CDSC
 
Descriptive Properties
FNCT (hrs)>1000ISO 16770, 4.0 MPa, 2% Arkopal N100, 80°C
MRS Classification (MPA)10ISO 9080
Odor Threshold<=2, EN 1622/EN 1420, measured on pellets/30°C/4 h extraction time
Processing Methodpipe, sheet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total Xsene® XS10 B HDPE, pipe, injection molding
Ethydco Advancene™ bEE-4906-AAH HDPE Pipe Extrusion
Borealis BorSafe™ HE3490-LS Black High Density Polyethylene for Pressure Pipes
Borealis BorSafe™ HE3490-LS-H HDPE Compound for Pressure Pipes
Chevron Phillips HiD® 9300 HDPE Orange Pipe Resin

PEQT8461 / 220096

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.