MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NYCOA ASN 27 300 KNF 30% Glass Fiber Reinforced, Heat Stabilized Nylon 6 Resin
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: NYCOA ASN 27 300 KNF is a 30% glass fiber reinforced, heat stabilized Nylon 6 resin used for injection molding. This grade features excellent strength and stiffness, dimensional stability, and a greater service life than standard grades of glass reinforced Nylon 6.

NYCOA ASN 27 300 KNF is available in UV stable, custom colors, and impact modified grades. It also has excellent chemical resistance to greases, oils, and other hydrocarbons.

Typical applications include automotive pedals, power tool housing, and lawn & garden equipment parts.

Information provided by Nycoa, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/ccASTM D792
Water Absorption 1.2 %24 hours; ASTM D570
Linear Mold Shrinkage 0.012 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.014 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ASTM D785
Tensile Strength, Yield 178 MPaASTM D638
Elongation at Break 3.0 %ASTM D638
Tensile Modulus 9.45 GPaASTM D638
Flexural Strength 210 MPaASTM D790
Flexural Modulus 8.22 GPaASTM D790
Izod Impact, Notched 135 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 222 °CASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 220 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °CASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Greene Tweed WR™ 575 PEEK, Bi-Directional Carbon Fiber Filled
Covestro Makrolon® 8035 Polycarbonate
Evonik VESTAKEEP® 2000 FC30 PEEK
Evonik VESTAKEEP® 2000 CF30 PEEK
Dow Questra® EA503 High Heat Syndiotactic Polystyrene, 30% Glass Filled

PNYCO10 / 55545

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.