MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema Rilsan® BMNO P20 TLD PA11
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 11 (PA11); Nylon 11, Unreinforced

Material Notes: Property data for dry samples, unless noted.

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccISO 1183
 1.05 g/ccCond.; ISO 1183
Water Absorption 1.8 %Dry; Sim. to ISO 62
Melt Flow 32 g/10 min
@Load 2.16 kg,
Temperature 235 °C
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 61
@Time 15.0 sec
Dry; ISO 7619-1
Tensile Strength, Yield 32.0 MPaCond.; ISO 527-1/-2
Elongation at Break >= 50 %Cond.; ISO 527-1/-2
Elongation at Yield 30 %Cond.; ISO 527-1/-2
Tensile Modulus 545 MPaCond.; ISO 527-1/-2
Charpy Impact Unnotched NB
@Temperature -30.0 °C
Cond.; ISO 179/1eU
 NB
@Temperature 23.0 °C
Cond.; ISO 179/1eU
Charpy Impact, Notched 7.00 kJ/m²
@Temperature -30.0 °C
Cond.; ISO 179/1eA
 NB
@Temperature 23.0 °C
Cond.; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmCond.; IEC 60093
Surface Resistance 2.00e+12 ohmCond.; IEC 60093
Dielectric Constant 3.0
@Frequency 1e+6 Hz
Dry; IEC 60250
 7.0
@Frequency 100 Hz
Dry; IEC 60250
Dielectric Strength 26.0 kV/mmCond.; IEC 60243-1
Dissipation Factor 0.0614
@Frequency 1e+6 Hz
Dry; IEC 60250
 0.19
@Frequency 100 Hz
Dry; IEC 60250
Comparative Tracking Index 600 VCond.; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 100 µm/m-°CDry; ISO 11359-1/-2
Melting Point 186 °C10°C/min; Dry; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 135 °CDry; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 47.0 °CDry; ISO 75-1/-2
Vicat Softening Point 145 °C50°C/h 50N; Dry; ISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 °CInjection Molding; ISO 294
Mold Temperature 50.0 °CInjection Molding; ISO 10724
Hold Pressure 16.0 MPaInjection Molding; ISO 294
 
Descriptive Properties
%Bio-Based92ASTM D6866
Bio-BasedYes
Form as DeliveredPellets
Heat StabilizedYes
Light StabilizedYes
Moisture SensitiveYes
PlasticizerYes
Processing MethodsInjection Molding
Release agentYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Rilsan® BMNO PA11
Arkema Rilsan® BECNO TL PA11
Arkema Rilsan® BMNO P40 TLD PA11
Arkema Rilsan® MB 3610 NAT PA11-I
Arkema Rilsan® BSR 30 PA11-CF30

PARKF899 / 193639

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.