MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultrason® S 3010 PSU
Categories: Polymer; Thermoplastic; Polysulfone (PSU)

Material Notes: Ultrason S 3010 is an unreinforced, higher viscosity injection molding and extrusion PSU grade, tougher and with improved chemical resistance. It conforms to FDA requirements of 21 CFR 177.1655.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccISO 1183
Water Absorption 0.80 %ISO 62
Moisture Absorption at Equilibrium 0.30 %23°C/50% R.H.; ISO 62
Viscosity Number 72 cm³/g
Linear Mold Shrinkage, Flow 0.0070 cm/cmISO 294
Linear Mold Shrinkage, Transverse 0.0074 cm/cmISO 294
Melt Flow 40 g/10 min
@Load 10.0 kg,
Temperature 360 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 135 MPaISO 2039-1
Tensile Strength at Break 75.0 MPa5mm/min; ISO 527-2
Tensile Strength, Yield 75.0 MPa50mm/min; ISO 527-2
 40.0 MPa
@Temperature 140 °C
 58.0 MPa
@Temperature 100 °C
 68.0 MPa
@Temperature 60.0 °C
 75.0 MPa
@Temperature 20.0 °C
Tensile Stress at Strain 20.0 MPa
@Strain 1 %,
Temperature 160 °C
ISO 527
 27.0 MPa
@Strain 1 %,
Temperature 23.0 °C
ISO 527
 35.0 MPa
@Strain 2 %,
Temperature 160 °C
ISO 527
 47.0 MPa
@Strain 2 %,
Temperature 23.0 °C
ISO 527
 70.0 MPa
@Strain 4 %,
Temperature 23.0 °C
ISO 527
Elongation at Break 5.7 %5mm/min; ISO 527-2
Elongation at Yield 5.7 %50mm/min; ISO 527-2
 0.50 %
@Time 3600 sec,
Pressure 10.0 MPa
ISO 899
 0.55 %
@Pressure 10.0 MPa,
Time 360000 sec
ISO 899
 0.56 %
@Pressure 10.0 MPa,
Time 3.60e+7 sec
ISO 899
 0.80 %
@Time 3600 sec,
Pressure 20.0 MPa
ISO 899
 0.90 %
@Pressure 20.0 MPa,
Time 360000 sec
ISO 899
 1.3 %
@Time 3600 sec,
Pressure 30.0 MPa
ISO 899
 1.4 %
@Pressure 30.0 MPa,
Time 360000 sec
ISO 899
 1.5 %
@Pressure 30.0 MPa,
Time 3.60e+7 sec
ISO 899
 1.9 %
@Time 3600 sec,
Pressure 40.0 MPa
ISO 899
 2.0 %
@Pressure 20.0 MPa,
Time 3.60e+7 sec
ISO 899
 2.0 %
@Pressure 40.0 MPa,
Time 360000 sec
ISO 899
 2.0 %
@Time 3600 sec,
Pressure 42.0 MPa
ISO 899
 2.2 %
@Pressure 42.0 MPa,
Time 360000 sec
ISO 899
 2.4 %
@Pressure 40.0 MPa,
Time 3.60e+7 sec
ISO 899
 2.5 %
@Pressure 42.0 MPa,
Time 3.60e+7 sec
ISO 899
Creep Strength 17.0 MPa
@Time 3.60e+7 sec
in water at 95°C
 20.0 MPa
@Time 3.60e+6 sec
in water at 95°C
 25.0 MPa
@Time 360000 sec
in water at 95°C
 32.0 MPa
@Time 36000 sec
in water at 95°C
Modulus of Elasticity 2.00 GPa
@Temperature 140 °C
ISO 527
 2.30 GPa
@Temperature 100 °C
ISO 527
 2.49 GPa
@Temperature 60.0 °C
ISO 527
 2.51 GPa
@Temperature 20.0 °C
ISO 527
Tensile Modulus 2600 MPaISO 527-2
Fatigue Strength 25.0 MPa
@# of Cycles 1.00e+7
 30.0 MPa
@# of Cycles 1.00e+6
 40.0 MPa
@# of Cycles 100000
 50.0 MPa
@# of Cycles 10000
Shear Modulus 0.0250 GPa
@Temperature 200 °C
ISO 6721
 0.800 GPa
@Temperature 175 °C
ISO 6721
 0.900 GPa
@Temperature 100 °C
ISO 6721
 0.950 GPa
@Temperature 50.0 °C
ISO 6721
Izod Impact, Notched (ISO) 5.50 kJ/m²ISO 180/A
 5.00 kJ/m²
@Temperature 120 °C
ISO 179/1eA
 6.00 kJ/m²
@Temperature -30.0 °C
ISO 180/A
 10.0 kJ/m²
@Temperature 50.0 °C
ISO 179/1eA
 13.0 kJ/m²
@Temperature -25.0 °C
ISO 179/1eA
Charpy Impact Unnotched NBISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 0.550 J/cm²ISO 179/1eA
 0.600 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
Tensile Creep Modulus, 1000 hours 2500 MPaISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 60093
Surface Resistance >= 1.00e+14 ohmIEC 60093
Dielectric Constant 3.1
@Frequency 100 Hz
IEC 60250
 3.1
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 37.0 kV/mmIEC 60243-1
Dissipation Factor 0.00080
@Frequency 100 Hz
IEC 60250
 0.0064
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 125 VTest Liquid A & B; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 53.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-1/-2
 60.0 µm/m-°C
@Temperature 140 - 180 °C
ISO 11359-1/-2
Maximum Service Temperature, Air 180 °Cshort cycle operations
Deflection Temperature at 1.8 MPa (264 psi) 175 °CISO 75-2
Glass Transition Temp, Tg 187 °CISO 11357-1/-2
UL RTI, Electrical 155 °C50% decrease of tensile strength after 20000h; 746B
Flammability, UL94 HB
@Thickness 1.60 mm
 V-2
@Thickness 3.20 mm
Oxygen Index 32 %ISO 4589-1/-2
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.63
Transmission, Visible 89 %
@Thickness 2.00 mm
ASTM D 1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 330 - 390 °CInjection molding
Mold Temperature 120 - 160 °CInjection molding
 
Compliance PropertiesOriginal ValueComments
FDA Yes21 CFR 177.1655
NSF YesNSF Std. 61
 
Descriptive Properties
ColorNatural
Commercial StatusNorth America and Europe
Impact ModifiedNo
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultrason® S 2010 PSU
BASF Ultrason® P 3010 PPSU Unreinforced Polyphenylsulfone
BASF Ultrason® S 6010 PSU
BASF Ultrason® S 2010 G6 30% Glass Filled PSU
BASF Ultrason® S 2010 G4 20% Glass Filled PSU

PBASF9408 / 85172

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.