MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI Type M10 Molybdenum High Speed Tool Steel (UNS T11310)
Categories: Metal; Ferrous Metal; Tool Steel

Material Notes: Used in high speed tool and cutting applications such as drills, milling processes, reamers, etc. Mo content promotes toughness, but requires more precise hardening conditions and caution about overheating.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.88 g/cc0.285 lb/in³
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.0 µm/m-°C
@Temperature 20.0 - 425 °C
6.11 µin/in-°F
@Temperature 68.0 - 797 °F
 11.9 µm/m-°C
@Temperature 20.0 - 540 °C
6.61 µin/in-°F
@Temperature 68.0 - 1000 °F
 12.4 µm/m-°C
@Temperature 20.0 - 650 °C
6.89 µin/in-°F
@Temperature 68.0 - 1200 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.84 - 1.05 %0.84 - 1.05 %
Chromium, Cr 3.75 - 4.5 %3.75 - 4.5 %
Copper, Cu <= 0.25 %<= 0.25 %
Iron, Fe 82.3 - 85.6 %82.3 - 85.6 %As Balance
Manganese, Mn 0.10 - 0.40 %0.10 - 0.40 %
Molybdenum, Mo 7.75 - 8.5 %7.75 - 8.5 %
Nickel, Ni <= 0.30 %<= 0.30 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si 0.20 - 0.45 %0.20 - 0.45 %
Sulfur, S <= 0.030 %<= 0.030 %0.06 to 0.15% may be specified to improve machinability
Vanadium, V 1.8 - 2.2 %1.8 - 2.2 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type M1 Molybdenum-Alloy High-Speed-Tool Steel (UNS T11301)
AISI Type M2 Molybdenum High Speed Tool Steel (UNS T11302)
AISI Type M3 Class 1 Molybdenum High Speed Tool Steel (UNS T11313)
AISI Type M41 Molybdenum High Speed Tool Steel (UNS T11341)
AISI Type H10 Chromium Hot Work Tool Steel (UNS T20810)

MSTM10 / 172265

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.