MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Carbon-Core Carbon Balsa Wood
Categories: Polymer; Renewable/Recycled Polymer; Wood and Natural Products; Wood

Material Notes: End Grain Balsa, a highly processed ultra light wood product, imparts impressive strength and stiffness to the sandwich panel. The end grain configuration of balsa provides high resistance to crushing, and is very difficult to tear apart. End grain balsa cored panels also have the ability to handle excessive dynamic loads with high resistance to fatigue. CarbonBalsa’s end-grain orientation gives it exceptional compression and shear properties. As an added benefit, CarbonBalsa provides good thermal and acoustic insulation. CarbonBalsa is select quality, kiln-dried, end-grain balsa wood suitable as a structural core material in composite sandwich construction. CarbonBalsa is a naturally renewable resource.

Information provided by Carbon-Core

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 9.00 - 10.0 lb/ft³
Water Absorption 9.66 %Average
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 1900 psiASTM C297
Compressive Strength 1895 psiASTM C365
Compressive Modulus 590000 psiASTM C365
Shear Modulus 23.1 ksiASTM C273
Shear Strength 432 psiASTM C273

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DIAB ProBalsa® PB Standard Balsa Wood
CoreLite BALSASUD® Core SG Standard Grade Balsa Core Material
3M Balsa Panels
CoreLite BALSASUD® Core UL Ultra Lite Balsa Core Material
CoreLite BALSASUD® Core HW Heavy Weight Balsa Core Material

PCARBC002 / 190821

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.