MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Abatron AboCast 10-5/AboCure 50-3 Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Cast, Unreinforced

Material Notes: AboCast 10-5 is a filled, high-viscosity epoxy resin. It is blended with AboCure 50-3 to make a structural adhesive and casting compound for the optic and electric industry. AboCure 50-3 is a clear room-temperature-cure, low-viscosity converter. AboCast 10-5/AboCure 50-3 has good adhesive, chemical, and physical properties. It is slow and easily pourable for casting. It is excellent for potting and encapsulation of delicate electronic components and general casting of small and large objects. It has versatile variable-ratio possibilities. This blend's main advantages are: it has low-viscosity and is room-temperature-cure, low exotherm, and thermocycling. It also is dielectric and offers good adhesion, virtually no shrinkage, and high resistance to alkalis, diluted acids, water, many solvents, and outdoors.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 85.0 °C
 
Processing PropertiesOriginal ValueComments
Pot Life 120 min
@Temperature 25.0 °C
100 g
 
Descriptive Properties
ColorGreen
Hardening Time (min)180 to 48025°C
Parts by Weight (pbw)100AboCast 10-5
 20-65AboCure 50-3
ViscosityFluid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Abatron AboCast 10-5/AboCure 3-4 Epoxy
Abatron AboCast 10-5/AboCure 50-12 Epoxy
Overview of materials for Thermoset Polyurethane, Liquid
Solvay Thornel® Mat VME Carbon Fiber
Overview of materials for Epoxy, Cast, Unreinforced

PABC802 / 107786

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.