MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bamberger Polymers Bapolene® 108A Low Density Polyethylene Film Extrusion Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Bapolene® 108A is a low density polyethylene for blown film applications and contains an antiblock additive. This product meets US FDA 21 CFR 177.1520.

Applications: Blown Film; Film; General Purpose; Packaging.

Information provided by Bamberger Polymers.

Key Words: Antiblocking; Food Contact Acceptable; Low Density
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.925 g/ccASTM D-1505
Thickness 50.8 micronsas tested; 2.5:1 BUR
Melt Flow 0.80 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D-1238
Antiblock Level 2500 ppmtarget
 
Mechanical PropertiesOriginal ValueComments
Dart Drop Test 120 gF50; ASTM D1709
Film Tensile Strength at Break, MD 29.65 MPaASTM D-882
Film Tensile Strength at Break, TD 22.75 MPaASTM D-882
1% Secant Modulus, MD 26000 psiASTM D882
1% Secant Modulus, TD 32000 psiASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 7.0 %ASTM D1003
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
processFilm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® 105F Low Density Polyethylene Film Resin
Bamberger Polymers Bapolene® 1030 Low Density Polyethylene Extrusion/Injection Resin
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
Mitsubishi Chemical Advanced Materials Proteus™ LDPE Low Density Polyethylene

PBP3B370Ch / 177295

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.