MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BiologiQ EcoStarch GS270 Thermoplastic Starch
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic

Material Notes: BiologiQ GS270 is a plasticized thermoplastic starch (TPS) called EcoStarch Resin (ESR). It is suitable for blending with petrochemical or bioresins where biobased content is desired. It Can be used as a stand alone polymer for certain low-temperature injection molding applications. It is highly compostable and biodegradable. It forms a crystalline structure product that has good strength and low plasticity. When GS270 absorbs moisture it exhibits plastic behavior and becomes flexible. When removed from humidity the material dries out and becomes crystalline again. Used for final products requiring plasticity such as plastic dinnerware, packaging. Blend with PE to make think film products like shopping bags.

Information provided by BiologiQ

Key Words: TPS, ESR, biopolymer, bioresin, biodegradeable
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccASTM D792
Melt Flow 1.98 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 30.0 MPaASTM D638
Tensile Strength, Yield >= 30.0 MPaASTM D638
Elongation at Break <= 10 %ASTM D638
Tensile Modulus 1.50 GPaASTM D638
Dart Drop Test 3500 gASTM D5628
 
Thermal PropertiesOriginal ValueComments
Melting Point 166 - 180 °CASTM D3418
Glass Transition Temp, Tg 81.0 - 100 °CASTM D3418
 
Processing PropertiesOriginal ValueComments
Drying Temperature 60.0 °C
Dry Time 1.00 - 4.00 hour
Moisture Content <= 1.0 %ASTM D6980

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Terraloy™ MB 10000A Thermoplastic Starch + LLDPE
Teknor Apex Terraloy™ BP 10000A Thermoplastic Starch + LLDPE
Teknor Apex Terraloy™ BP 20001A Thermoplastic Starch + Copolyester
Teknor Apex Terraloy™ MB 13000A Thermoplastic Starch + PP
Teknor Apex Terraloy™ BP 13000A Thermoplastic Starch + PP

PBIOLQ01 / 176019

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.