MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite Durez® 17983 Phenolic Resin
Categories: Polymer; Thermoset; Phenolic

Material Notes: Durez® 17983 is a water-soluble, phenol-formaldehyde liquid resin of the one-step type, having a limited water tolerance butcapable of self-emulsification when its water tolerance is exceeded. The resin is recommended for treating paper, wood and organic and inorganic fibres to improve strength, moisture resistance and impart other desirable properties, and is suitable for both direct treating and better addition processes.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 69 %
@Load 0.00100 kg,
Temperature 135 °C
1 hr; DCT 156
Solubility in Water 100 %DCT 325
Viscosity Measurement 500
@Temperature 25.0 °C
DCT 61

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bakelite® PF 1141 Phenolic Formaldehyde Resin, High Surface Quality, Resistant to High Temperatures, Dishwasher Proof
Celanese Butoxyl® 50000872 3-Methoxy-n-Butylacetate
Sumitomo Bakelite Durez® 31513 Phenolc Resin
Bakelite® MP 4165 Melamine Phenolic Resin, Copper Adhesive, Low Shrinkage, High Mechanical Strength
Chemours Teflon® PFA Grade 940 HP Plus Extrusion and Molding Resin

PSUMIT231 / 194036

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.