MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemical Concepts Chem-Set™ 738 General Purpose Hot Melt Adhesive
Categories: Polymer; Adhesive; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: A light brown hot melt adhesive for woodworking and carpets. (15 second open time) A light brown hot melt adhesive for woodworking and carpets. Low viscosity. Good hot tack.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 100 %
Viscosity 2080 cP
@Temperature 191 °C
 4310 cP
@Temperature 163 °C
 17100 cP
@Temperature 121 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 119 °FPeel Adhesion Failure. ASTM D4498, 45# Kraft paper substrates, 100 g weights.
Flash Point >= 450 °F
Shear Adhesion Failure Temperature 170 °F45# Kraft paper substrates, 500 g weights; ASTM D4498
 
Processing PropertiesOriginal ValueComments
Processing Temperature 250 - 380 °FApplication
 
Descriptive Properties
Chemical CompositionEthylene Vinyl Acetate
ColorAmber
Mettler Softening Point205°F. ASTM D6493-99
Odorslight
Open Time15 sec. ASTM D4497-94(1999) using 45# Kraft paper substrates

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chosun Refractories CUN-738 Nozzle Brick
Solvay BR® 127 Primer with FM 73 Adhesive
IN-738 Cast Nickel Superalloy
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
Chemical Concepts Chem-Set™ 711 Fast Set Hot Melt Adhesive

PCHEMI928 / 232212

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.