MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Industeel URANUS® B28 High Nickel Super-Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes: Description: URANUS® B28 (UR B28) is a super-austenitic stainless steel with very high nickel (31%) and chromium (27%) contents. The molybdenum content is about 3.5%. The alloy is designed for specific purposes, including sulphuric or phosphoric acid applications. It behaves particularly well in sulphuric and phosphoric acid environments, even when contaminated by chlorides and fluorides species. The high nickel content improves its stress corrosion cracking resistance. The combined chromium and molybdenum additions contribute to increase the localized corrosion resistance. The alloy behaves much better than alloy 825 and could be considered in some applications (sour gas) to replace the more expensive 625 grade. The alloy is extensively used in chemical and offshore applications including very sour gas fields.

Information provided by manufacturer.

Key Words: EURONORM X1 Ni Cr Mo Cu 31.27.4, AFNOR Z2 NCDU 31.27.03, DIN W. Nr 1.4563, UNS N08028
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 250 - 310Typical, V10
Tensile Strength, Ultimate >= 500 MPaMinimum Guaranteed
Tensile Strength, Yield >= 220 MPa
@Strain 0.2 %
 >= 250 MPa
@Strain 1 %
Elongation at Break >= 40 %
Modulus of Elasticity 195 GPa
Poissons Ratio 0.30Calculated
Shear Modulus 75.0 GPa
@Temperature 20.0 °C
Charpy Impact >= 100 J
@Temperature -196 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000100 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.8 µm/m-°C
@Temperature 20.0 - 200 °C
 16.5 µm/m-°C
@Temperature 20.0 - 300 °C
 17.3 µm/m-°C
@Temperature 20.0 - 500 °C
Specific Heat Capacity 0.450 J/g-°C
@Temperature 20.0 °C
Thermal Conductivity 12.0 W/m-K
@Temperature 20.0 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.020 %
Chromium, Cr 27 %
Copper, Cu 1.0 %
Iron, Fe 37.43 - 37.45 %As remainder
Molybdenum, Mo 3.5 %
Nickel, Ni 31 %
Nitrogen, N 0.050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Industeel URANUS® 52N+ 25 Cr Super Duplex Stainless Steel with PREN = 40
Special Metals INCOLOY® 25-6HN Super-Austenitic Stainless Steel
Special Metals INCOLOY® 25-6MO Super Austenitic Stainless Steel (UNS N08926)
Special Metals INCONEL® Alloy X-750
Alloy Wire International RW 80 Ni-Cr Resistance Wire

NINDUST44 / 17582

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.