MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Glass Fiber Filled

Material Notes: Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties remain constant after moisture absorption up to a temperature of 60°C [140°F], for instance, for automotive valve housings.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.43 g/ccISO 1183
Moisture Absorption at Equilibrium 0.80 - 1.2 %23°C; 50% RH; ISO 62
Water Absorption at Saturation 4.3 - 5.3 %ISO 62
Viscosity Measurement 130ISO 307
Linear Mold Shrinkage 0.0033 cm/cmrestricted
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 200 MPa50 mm/min; ISO 527-1/-2
Modulus of Elasticity 12.0 GPaISO 527-1/-2
Tensile Creep Modulus, 1000 hours 8700 MPa
@Strain <=0.5 %
ISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmIEC 60093
 1.00e+8 ohm-cm
@Temperature 140 °C
IEC 60093
 2.00e+10 ohm-cm
@Temperature 100 °C
IEC 60093
 1.00e+11 ohm-cm
@Temperature 80.0 °C
IEC 60093
 5.00e+11 ohm-cm
@Temperature 60.0 °C
IEC 60093
 1.00e+13 ohm-cm
@Temperature 40.0 °C
IEC 60093
 1.00e+15 ohm-cm
@Temperature 20.0 °C
IEC 60093
Surface Resistance 1.00e+12 ohmIEC 60093
Dielectric Constant 4.4
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.030
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VTest solution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.30 J/g-°C
Thermal Conductivity 0.280 W/m-KDIN 52612
Melting Point 295 °CDIN 53765
Maximum Service Temperature, Air 135 °Cfor 50% loss of tensile strength after 20000hr
 160 °Cfor 50% loss of tensile strength after 5000hr
 270 °C
 
Processing PropertiesOriginal ValueComments
Melt Temperature 310 - 330 °CInjection-molding/Extrusion
Mold Temperature 80.0 - 120 °CInjection-molding
 
Descriptive Properties
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® A3WG6 BK 00564 30% Glass Filled PA66 (Conditioned)
Adell AD-30 Nylon 66, Ultra High Impact
Clariant Renol PA121 Nylon 66, Impact Modified
BASF Ultramid® A3L HP BK20465 PA66 (Conditioned)
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry)

PBASG0291 / 131924

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.