MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite Sumikon® PM-9610 Phenolic, Compression Grade
Categories: Polymer; Thermoset; Phenolic; Phenolic/Glass Fiber SMC

Material Notes: Durez “SUMIKON” PM-9610 black Phenolic is a two stage glass and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and higher dimensional stability with excellent heat resistance. Typical applications include brush holders for high temperature, and timing pulleys.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.02 g/ccASTM D792
Apparent Bulk Density 0.960 g/ccASTM D1895
Water Absorption 0.030 %ASTM D570
Linear Mold Shrinkage 0.0030 in/inASTM D6289
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 90.0 MPaASTM D638
Tensile Modulus 25.5 GPaASTM D638
Flexural Strength 131 MPaASTM D790
Compressive Strength 241 MPaASTM D695
Izod Impact, Notched 21.4 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmASTM D257
Dielectric Constant 4.9
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 9.80 kV/mmStep by Step; ASTM D149
 14.9 kV/mmShort Time; ASTM D149
Dissipation Factor 0.030
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 204 °CASTM D648
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sumitomo Bakelite Sumikon® PM-6630 Type Black Phenolic Novolac
Sumitomo Bakelite Sumikon® PM-6830 Type Black Phenolic Resol
Sumitomo Bakelite Sumikon® PM-9501 Type J Black Phenolic Novolac

PSUMIT488 / 194293

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.