MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TechnylStar™ S 60G1 V30 PA6, 30% glass filled, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Description: TECHNYLSTAR™ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized and provides optimized injection moulding performance. This product is available in natural, grey & black colors as standard and can be made in other specific colors upon request.

Benefits: This product offers excellent flame retardancy properties (UL 94, 5VA, GWIT) combined with best in class processing, mechanical and electrical performance.

Available in: Asia Pacific, Europe, Latin America and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

Applications: This product is ideally suited for power distribution, industrial control and appliance applications such as MCBs and contactors, as well as being able to be used in many varied thin wall applications where its high flow polymer base enables it to achieve a UL94 V-0 rating down to a 0.4mm wall thickness.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.42 g/ccISO 1183/A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 97.0 MPaISO 527 Type 1A
Elongation at Break 5.1 %ISO 527 Type 1A
Tensile Modulus 8500 MPaISO 527 Type 1A
Flexural Strength 175 MPaISO 178
Flexural Modulus 7100 MPaISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²ISO 180/1eA
Izod Impact, Unnotched (ISO) 63.0 kJ/m²ISO 180/1eU
Charpy Impact Unnotched 70.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 12.5 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.35IEC 60250
Dielectric Strength 23.0 kV/mmIEC 60243
Dissipation Factor 0.080IEC 60250
Comparative Tracking Index 600 VSolution A; IEC 60112
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TechnylStar™ S 60G1 V30 PA6, 30% glass filled, DRY
Domo TechnylStar™ S 60G1 V30 30% Glass Reinforced Nylon 6, Flame Retardant
Trinseo TYRIL™ 875 SAN Resin
Envalior Pocan® BF 4130 XF 000000 PBT, 30% Glass Fiber
Envalior Pocan® AF 4130 000000 PBT, 30% Glass Fiber Reinforced

PRHOD838 / 138069

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.