MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Vandar® 2100UV PBT, Impact Modified
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified

Material Notes: Vandar 2100UV is a polyester alloy designed to offer maximum impact strength at room and low temperatures. This unfilled compound is characterized by outstanding chemical resistance, dimensional stability, paintability, and toughness. Vandar 2100UV is available in UV stable colors.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.23 g/ccASTM D792
Density 1.216 g/ccISO 1183
Water Absorption 0.10 %
@Temperature 22.8 °C
24hr immersion; ASTM D570
Moisture Absorption 0.200 %23°C/50%RH; ISO 62
Linear Mold Shrinkage, Flow 0.018 cm/cmASTM D955
 0.017 - 0.022 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.017 - 0.022 cm/cmISO 294-4
Melt Flow 5.5 g/10 min
@Load 5.00 kg,
Temperature 250 °C
[cm3/10min]; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 38ISO 2039-2
Tensile Strength at Break 29.0 MPa50mm/min; ISO 527-2/1A
Tensile Strength, Yield 38.0 MPa50mm/min; ISO 527-2/1A
 6300 psiASTM D638
Tensile Stress at Strain 26.0 MPa
@Strain 50 %
ISO 527-2/1A
Elongation at Break 150 %ASTM D638
 174 %
 247 %50mm/min; ISO 527-2/1A
Elongation at Yield 4.4 %50mm/min; ISO 527-2/1A
Tensile Modulus 1763 MPa50mm/min; ISO 527-2/1A
Flexural Strength 47.0 MPaISO 178
 8700 psiASTM D790
Flexural Modulus 1674 MPaISO 178
 280000 psiASTM D790
Izod Impact, Notched 99.0 ft-lb/inASTM D256
 3.00 ft-lb/in
@Temperature -28.9 °C
ASTM D256
Izod Impact, Notched (ISO) NBISO 180/1A
Charpy Impact Unnotched NBISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 80.0 kJ/m²ISO 179/1eA
 19.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohmIEC 60093
Dielectric Constant 3.6
@Frequency 1e+6 Hz
IEC 60250
 4.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 24.0 kV/mmIEC 60243-1
Dissipation Factor 0.0070
@Frequency 100 Hz
IEC 60250
 0.020
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 130 µm/m-°CISO 11359-2
Melting Point 225 °C10°C/min; ISO 11357-1,-2,-3
 437 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 86.0 °CISO 75-1, -2
 220 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 51.0 °CISO 75-1, -2
 120 °FASTM D648
Vicat Softening Point 128 °CISO 306
Glass Transition Temp, Tg 60.0 °CISO 11357-1,-2,-3
Flammability, UL94 HB
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 65.0 - 96.0 °Ccavity
 250 - 260 °Chot runner
Feed Temperature 230 - 240 °C
Zone 1 230 - 240 °C
Zone 2 235 - 250 °C
Zone 3 235 - 250 °C
Zone 4 240 - 260 °C
Die Temperature 240 - 260 °C
Melt Temperature 235 - 260 °C
 260 °CISO 294
Mold Temperature 82.0 °CISO 294
Injection Velocity 300 mm/secISO 294
Drying Temperature 120 - 130 °C
Dry Time 4.00 hour
Moisture Content <= 0.020 %
Hold Pressure 86.0 MPaISO 294
 
Descriptive Properties
Injection moldingYes
Injection speedmedium-fast
Processing conditions acc. ISO7792-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Nilit FRIANYL A63 HS28 Nylon 6.6 for injection molding
Celanese Vandar® 2100 PBT, Unfilled
Americhem Engineered Compounds ColorFast® PCT2014 PC/PBT Alloy
Celanese Celanex® 3300-2LM PBT, Glass Reinforced
Celanese Celanex® 3226 PBT, Glass Reinforced

PHCQ474 / 178929

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.