MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Adflex 7634 XCP Thermoplastic Polyolefin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyolefin

Material Notes: Adflex 7634 XCP is developed for the central layer of tough, transparent co-extruded cast-film structures. It combines transparency with high softness, a very high toughness even at low temperatures and an excellent compatibility with other polyolefins. It does not contain any slip nor anti-blocking agents. Typical applications of the Adflex 7634 XCP are co-extruded cast-film for food packaging, hygiene applications, surface protection where the outside layer can be any polyolefin homo or copolymer. Commercial: Active. Availability: Africa-Middle East; Asia-Pacific; Australia and New Zealand; Europe; North America; South & Central America. Application: Bags & Pouches; Barrier Film; Breathable Film; Film Wrap; Food Packaging Film; Lamination Film; Peelable Film; Stationery Film Market Flexible Packaging; Rigid Packaging. Processing Method: Blown Film; Cast Film; Extrusion Blow Molding; Extrusion Coating; Injection Molding; Thermoforming. Attribute: Good Toughness; High Clarity; Low Temperature Toughness; Soft.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.880 g/cc0.0318 lb/in³ISO 1183-1
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 3838ISO 868
Tensile Strength, Yield 8.00 MPa1160 psiISO 527-1,-2
Elongation at Break 600 %600 %ISO 527-1,-2
Flexural Modulus 0.200 GPa29.0 ksiISO 178
Charpy Impact Unnotched  1.50 J/cm²
@Temperature -20.0 °C
7.14 ft-lb/in²
@Temperature -4.00 °F
ISO 179
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 40.0 °C104 °Funannealed; ISO 75B-1,-2
Vicat Softening Point 85.0 °C185 °FA/50N; ISO 306
 
Descriptive Properties
Processing MethodBlown Film; Cast Film; Extrusion Blow Molding; Extrusion Coating; Injection Molding; Thermoforming

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
United Cast Bar Unibar 700-2 Continuously Cast Spheroidal Graphite Iron
Silver, Ag
LyondellBasell Dexflex 1066-UV YGYA Thermoplastic Polyolefin
LyondellBasell Adflex Q 300F Thermoplastic Polyolefin
LyondellBasell Adflex C 200F Thermoplastic Polyolefin

PEQT7001 / 218640

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.