MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Denka REOMER G G8082 Thermoplastic Elastomer, For Injection Molding  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive distortion, rebound elasticity, etc. compared to soft PVC, and excellent bending strength and ozone resistance compared to rubber

Applications

[Automotive components]

  • door moldings
  • weather-strips
  • glass run channels
  • side bumpers
  • gaskets
  • mud flaps
  • head rests
  • arm rests
  • steering wheels
  • trim
  • shift bar boots
  • pedal pads
[Construction material, manufacturing article home electric, appliance components]
  • gaskets
  • airtight materials
  • container packing
  • packing for vacuum cleaners
  • hoses
  • tubes
[For electric wire]
  • appliance cords
  • cabtire

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/ccJIS-Z-8807
Evaporation Loss 5.0 %JIS-A-5756
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 82JIS-K-6301
Tensile Strength at Break 21.68 MPaJIS-K-6723
Elongation at Break 320 %JIS-K-6723
100% Modulus 0.012753 GPa
@Strain 100 %
JIS-K-6723
Resilience 21JIS-K-6301
Compression Set 54 %JIS-K-6301
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air -27.0 °CJIS-K-6723
 
Descriptive Properties
Bending Strength, Times, JIS-K-6301100k
Heating: Retention Rate of Elongation, %80100°C x 120 hrs
Heating: Retention Rate of Tensile Strength, %107100°C x 120 hrs
Oil Resistance: Retention of Tensile Strength, %93JIS-K-6723
Oil Resistance: Retention Rate of Elongation, %72JIS-K-6723

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyester Thermoplastic Elastomer
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber
Celanese Hytrel® 7246 TPC-ET
Denka LCS Z1075 Thermoplastic Elastomer, Extrusion grade (general)
Denka LCS Z1050 Thermoplastic Elastomer, Extrusion grade (general)

PDENK103 / 29767

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.