MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Rogers Arlon CLTE-AT Commercial Ceramic PTFE
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.

CLTE-AT is a micro-dispersed ceramic PTFE composite utilizing a woven fiberglass reinforcement to provide the highest degree of stability, critical in multi-layer designs.

  • Ceramic/PTFE microwave composite
  • Mechanically more robust and more dimensionally stable than alternatives
  • High thermal conductivity
  • Lowest Insertion Loss in commercial class
  • Very low Loss Tangent (0.0013)
  • Tight Dielectric constant and Thickness tolerance
  • Electrical phase stability vs. temperature

Benefits:

  • Excellent thermal stability of Dk and Df
  • Phase stability across temperature
  • High degree of Dimensional stability required for complex, multi-layer boards
  • Excellent CTE in X, Y and Z

Typical Applications:

  • Automotive Radar & Adaptive Cruise Control Applications
  • Microwave/RF Applications
  • Phase/Temperature Sensitive Antennas
  • Phase Sensitive Electronic Applications
  • RF and Microwave Filters

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: Arlon Materials for Electronics (MED) is a major manufacturer of specialty high performance laminate and prepreg materials for use in a wide variety of printed circuit board (PCB) applications and in several distinctive markets.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.06 g/ccASTM D792 Method A
Water Absorption 0.030 %IPC TM-650 2.6.2.1
Outgassing - Total Mass Loss 0.00 %
@Pressure <=1.33e-10 MPa,
Temperature 125 °C
Water Vapor Recovered; NASA SP-R-0022A
 0.040 %
@Pressure <=1.33e-10 MPa,
Temperature 125 °C
NASA SP-R-0022A
Collected Volatile Condensable Material 0.00 %
@Pressure <=1.33e-10 MPa,
Temperature 125 °C
NASA SP-R-0022A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 4400 psiCross; IPC TM-650 2.4.18.3
 7000 psiMachine; IPC TM-650 2.4.18.3
Modulus of Elasticity 260 ksiIPC TM-650 2.4.18.3
Flexural Strength 7.80 ksiCross; IPC TM-650 2.4.4
 14.6 ksiMachine; IPC TM-650 2.4.4
Compressive Modulus 244 ksiASTM D3410
Poissons Ratio 0.17ASTM D3039
Shear Modulus 0.760 GPaCalculated
Peel Strength 7.00 pliTo Copper (1 oz./35 micron); After Process Solutions; IPC TM-650 2.4.8
 7.00 pliTo Copper (1 oz./35 micron); After Thermal Stress; IPC TM-650 2.4.8
 9.00 pliTo Copper (1 oz./35 micron); At Elevated Temperatures; IPC TM-650 2.4.8.2
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.25e+14 ohm-cmC96/35/90; IPC TM-650 2.5.17.1
Surface Resistance 2.02e+14 ohmC96/35/90; IPC TM-650 2.5.17.1
Dielectric Constant 3.0
@Frequency 1e+10 Hz
IPC TM-650 2.5.5.3
Dielectric Breakdown 58000 VIPC TM-650 2.5.6
Dissipation Factor 0.00125
@Temperature -20.0 °C
 0.014
@Temperature 120 °C
 0.0013
@Frequency 1e+6 Hz
IPC TM-650 2.5.5.3
 0.0013
@Frequency 1e+10 Hz
IPC TM-650 2.5.5.5
Arc Resistance 250 secIPC TM-650 2.5.1
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.00 µm/m-°C
@Temperature 50.0 - 150 °C
IPC TM-650 2.4.41
CTE, linear, Transverse to Flow 20.0 µm/m-°C
@Temperature 50.0 - 150 °C
z direction; IPC TM-650 2.4.24
Thermal Conductivity 0.640 W/m-KASTM E1461
Decomposition Temperature 487 °COnset; IPC TM-650 2.4.24.6
 529 °C5 percent; IPC TM-650 2.4.24.6
Flammability, UL94 V-0
 
Descriptive Properties
IPC Delamination - T260 (minutes)> 60IPC TM-650 2.4.24.1
IPC Delamination - T288 (minutes)> 60IPC TM-650 2.4.24.1
IPC Delamination - T300 (minutes)> 60IPC TM-650 2.4.24.1
Temperature Coefficient of Dielectric (ppm/°C)-10IPC TM-650 2.5.5.5; at 10 GHz (-40 - 150°C)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Rogers Arlon CLTE-XT High Precision Ceramic PTFE
Quadrant Symalit® PVDF (ASTM Product Data Sheet)
Isoflon PTFE + 15% Ceramic Polytetrafluoroethylene with 15% Ceramic
Isoflon Teflon® 20 AD Polytetrafluoroethylene Film
Mitsubishi Chemical Advanced Materials Fluorosint™ 135 PTFE and PPS Blend, with Proprietary Lubrication Fillers

PARLM9866 / 149019

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.