MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition A
Categories: Metal; Ferrous Metal; Martensitic; Stainless Steel; Precipitation Hardening Stainless

Material Notes: AK Steel 15-5 PH® provides high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, low-temperature heat treatments minimize distortion and scaling. AK Steel 15-5 PH® is the ferrite-free version of AK Steel 17-4 PH® Stainless Steel. Both alloys are widely used in the aerospace, chemical, petrochemical, food processing, paper and general metalworking industries.

The material supplied from the mill is in Condition A. After fabrication eight standard heat treatments have been developed to provide a wide range of properties.

Information provided by AK Steel

Key Words: UNS S15500
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.78 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 35Longitudinal
 35Transverse
Tensile Strength, Ultimate 1110 MPaLongitudinal
 1116 MPaTransverse
Tensile Strength, Yield 963 MPa
@Strain 0.2 %
Longitudinal
 988 MPa
@Strain 0.2 %
Transverse
Elongation at Break 7.6 %in 2 inches, Transverse
 8.4 %in 2 inches, Longitudinal
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.8 µm/m-°C
@Temperature 21.0 - 93.0 °C
 11.3 µm/m-°C
@Temperature <=427 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.070 %
Chromium, Cr 14 - 15.5 %
Copper, Cu 2.5 - 4.5 %
Iron, Fe 71.91 - 79.85 %As Remainder
Manganese, Mn <= 1.0 %
Nb + Ta 0.15 - 0.45 %
Nickel, Ni 3.5 - 5.5 %
Phosphorus, P <= 0.040 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition A
AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition H 900
AISI Type S15500 (15Cr-5Ni) Precipitation Hardening Stainless Steel transverse direction, condition H900
Overview of materials for Precipitation Hardening Stainless
Overview of materials for T 400 Series Stainless Steel

NAKS116 / 14719

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.