Dow DNDA-1082 NT 7 Linear Low Density Polyethylene Resin
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
Linear Low Density (LLDPE)
Material Notes:
DOW DNDA-1082 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids.
Information provided by Dow
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.933
g/cc
0.0337
lb/in³
ASTM D792
Melt Index of Compound
155
g/10 min
@Load 2.16 kg,
Temperature 190 °C
155
g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Shore D
52
52
Molded and tested in accordance with ASTM D4976; ASTM D2240
Tensile Strength at Break
8.96
MPa
1300
psi
Molded and tested in accordance with ASTM D4976; ASTM D638
Tensile Strength, Yield
16.5
MPa
2400
psi
Molded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Break
50 %
50 %
Molded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Yield
8.0 %
8.0 %
Molded and tested in accordance with ASTM D4976; ASTM D638
Flexural Modulus
0.572
GPa
@Strain 2 %
83.0
ksi
@Strain 2 %
Secant; Molded and tested per ASTM D4976; ASTM D790 B
Tensile Impact Strength
105
kJ/m²
50.0
ft-lb/in²
Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S
Thermal Properties
Metric
English
Comments
Melting Point
125
°C
257
°F
Dow Method (DSC)
Crystallization Temperature
113
°C
235
°F
Dow Method (DSC)
Deflection Temperature at 0.46 MPa (66 psi)
52.2
°C
126
°F
Molded and tested in accordance with ASTM D4976; ASTM D648
Vicat Softening Point
122
°C
252
°F
ASTM D1525
Brittleness Temperature
-20.0
°C
-4.00
°F
Molded and tested in accordance with ASTM D4976; ASTM D746
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
NOVA Chemicals Surpass® IFs932-R Octene SLLDPE Injection Molding Resin
LyondellBasell Petrothene® GA594189 Linear Low Density Polyethylene, Injection Molding Grade
Dow DNDA-1081 NT 7 Linear Low Density Polyethylene Resin
LyondellBasell Petrothene® GA694189 Linear Low Density Polyethylene, Injection Molding Grade
Dow DNDA-1149 NT 7 Linear Low Density Polyethylene Resin
PDOW1269 / 30487
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.