MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Dow DNDA-1082 NT 7 Linear Low Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: DOW DNDA-1082 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.933 g/ccASTM D792
Melt Index of Compound 155 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 52Molded and tested in accordance with ASTM D4976; ASTM D2240
Tensile Strength at Break 1300 psiMolded and tested in accordance with ASTM D4976; ASTM D638
Tensile Strength, Yield 2400 psiMolded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Break 50 %Molded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Yield 8.0 %Molded and tested in accordance with ASTM D4976; ASTM D638
Flexural Modulus 83000 psi
@Strain 2 %
Secant; Molded and tested per ASTM D4976; ASTM D790 B
Tensile Impact Strength 50.0 ft-lb/in²Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S
 
Thermal PropertiesOriginal ValueComments
Melting Point 257 °FDow Method (DSC)
Crystallization Temperature 113 °CDow Method (DSC)
Deflection Temperature at 0.46 MPa (66 psi) 126 °FMolded and tested in accordance with ASTM D4976; ASTM D648
Vicat Softening Point 252 °FASTM D1525
Brittleness Temperature -4.00 °FMolded and tested in accordance with ASTM D4976; ASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NOVA Chemicals Surpass® IFs932-R Octene SLLDPE Injection Molding Resin
LyondellBasell Petrothene® GA594189 Linear Low Density Polyethylene, Injection Molding Grade
Dow DNDA-1081 NT 7 Linear Low Density Polyethylene Resin
LyondellBasell Petrothene® GA694189 Linear Low Density Polyethylene, Injection Molding Grade
Dow DNDA-1149 NT 7 Linear Low Density Polyethylene Resin

PDOW1269 / 30487

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.