MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Aptek 2712-A/B Very low stress silicone adhesive
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Very low stress silicone adhesive; -110ºC to 260ºC operating range; Low outgassing/space grade
APTEK 2712-A/B is a two component, white, very soft, thixotropic, electrically insulative, silicone adhesive displaying excellent flow temperature flexibility and unusually high physical strength properties. APTEK 2712-A/B has been designed to fully cure at room temperature and can be accelerated with a brief low temperature cure. This 100% solid system has been manufactured with highly pure resins to minimize the occurrence of ionic contamination without outgassing during cure or service.

Very flexible/low modulus over wide temperature range to absorb stress build-up during thermal cycling; Convenient 1:1 PBW or PBV mix ratio for easy handling-ideal for cartridge dispensers/repair kits; Very good adhesion to various substrates when used in conjunction with APTEK P-107 primer; Long work life, short cure cycle options for improved productivity on large area bonding applications.

APTEK 2712A is a white silica-filled silicone resin blend. APTEK 2712B is a translucent silica-filled silicone resin blend.

Information provided by Aptek Laboratories, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³A Component; ASTM D1475
 1.15 g/cc0.0415 lb/in³B Component; ASTM D1475
Outgassing - Total Mass Loss 0.55 %0.55 %at 10E-6 torr; ASTM E595
Collected Volatile Condensable Material 0.050 %0.050 %at 10E-6 torr; ASTM E595
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 1616Cured property; ASTM D2240
Tensile Strength, Ultimate 4.14 MPa
@Thickness 1.47 mm
600 psi
@Thickness 0.0580 in
Cured; ASTM D638
Elongation at Break 700 %700 %Cured property; ASTM D638
Adhesive Bond Strength 2.76 MPa400 psiAl-to-Al Lap Shear; Cured property;5 mil bondline thickness on primed aluminum panels; ASTM D1002
Tear Strength 23.7 kN/m135 pliASTM D624
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmCured property; ASTM D257
Dielectric Strength 13.8 kV/mm
@Thickness 6.35 mm
350 kV/in
@Thickness 0.250 in
Cured; ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear  54.0 µm/m-°C
@Temperature 20.0 °C
30.0 µin/in-°F
@Temperature 68.0 °F
Cured property; alpha 1
 235 µm/m-°C
@Temperature 20.0 °C
131 µin/in-°F
@Temperature 68.0 °F
Cured property; alpha 2
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -110 °C-166 °F
Glass Transition Temp, Tg -110 °C-166 °FCured property; Perkin Elmer TMS-2
Flash Point >= 150 °C>= 302 °FA Component; ASTM D92
 >= 150 °C>= 302 °FB Component; ASTM D92
 
Processing PropertiesMetricEnglishComments
Processing Temperature 25.0 °C77.0 °FCure Time not defined
 65.0 °C149 °FCure 1 hrs
 100 °C212 °FCure 0.5 hrs.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CHT Group AS1802 (1084G) SILCOTHERM 1 Part RTV silicone adhesive
Elkem (Bluestar Silicones) BLUESIL™ RTV 3611 A/B Silicone Rubber
Humiseal 1C49 Silicone Conformal Coating
Humiseal 1C51 Silicone Conformal Coating
Humiseal 1C55 Silicone Conformal Coating

PAPTEK07 / 24169

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.