MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cosmic Plastics K43/6260 Mineral Filled Diallyl Iso-Phthalate Molding Compound  (discontinued **)
Categories: Polymer; Thermoset; Diallyl Phthalate (DAP); Diallyl Phthalate (DAP), Cast, Mineral Filler

Material Notes: Description: Cosmic K43 / 6260 is a mineral filled, general purpose diallyl iso-phthalate molding compound which is supplied in a granular form. It pours easily, can be preformed, and molds easily in standard compression, transfer or injection equipment.

Features: K43 / 6260 has ultra high heat resistance, exceptionally high arc resistance and is easy to mold around inserts.

Applications: K43 / 6260 has ultra high heat resistance, exceptionally high arc resistance and is easy to mold around inserts.

Information provided by Cosmic Plastics Inc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.80 g/cc
Bulk Factor 2.3
Water Absorption 0.40 %
@Temperature 50.0 °C,
Time 173000 sec
Linear Mold Shrinkage 0.0030 - 0.0070 in/in
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 4500 - 6000 psi
Flexural Strength 10000 - 13000 psi
Compressive Strength 20000 - 32000 psi
Izod Impact, Notched 0.250 - 0.500 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cm
 6.00e+9 ohm-cm
@Temperature 70.0 °C,
Time 2.59e+6 sec
100% RH
Surface Resistance >= 1.00e+16 ohm
 1.00e+10 ohm
@Temperature 70.0 °C,
Time 2.59e+6 sec
100% RH
Dielectric Constant 4.0
@Frequency 1e+6 Hz
Dry
 4.0
@Frequency 1e+6 Hz
Wet
 4.6
@Frequency 1000 Hz
Dry
 4.7
@Frequency 1000 Hz
Wet
Dielectric Strength 360 V/milWet, step by step
 400 V/milDry, step by step
Dielectric Breakdown 48 VWet, step by step
 55 VDry, step by step
Dissipation Factor 0.031
@Frequency 1e+6 Hz
Dry
 0.035
@Frequency 1000 Hz
Dry
 0.039
@Frequency 1e+6 Hz
Wet
 0.043
@Frequency 1000 Hz
Wet
Arc Resistance 180 sec
 
Thermal PropertiesOriginal ValueComments
CTE, linear 46.0 µm/m-°C
@Temperature -40.0 - 100 °C
Heat Distortion Temperature 260 °C
 
Processing PropertiesOriginal ValueComments
Mold Temperature 135 - 170 °C
 
Descriptive Properties
Dimensional Stability<0.08%
MIL-M-14MDG6260, ASTM D5948-96
 MIGK43, ASTM D5948-96
Molding Pressure500-8000 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sumitomo Bakelite RX® 643 Phenolic Resole Compound
Sumitomo Bakelite RX® 647 Phenolic Resole Compound
Cosmic Plastics D44 Mineral Filled Diallyl Iso-Phthalate Molding Compound
Sumitomo Bakelite North America RX® 640 Fiberglass Reinforced Phenolic Resole
Cosmic Plastics K31/6220 Short Glass Fiber Filled Diallyl Iso-Phthalate Molding Compound

PCOSM012 / 190794

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.