MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röhm Plexiglas® df23 8N Molding Compound
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, General Purpose, Molded

Material Notes: Description: PLEXIGLAS® df21 8N, PLEXIGLAS® df22 8N and PLEXIGLAS® df23 8N molding compounds based on PLEXIGLAS® 8N are characterized by diffuse scattering of light. Besides showing the familiar properties of standard PLEXIGLAS® molding compound, such as
  • excellent weatherability
  • high surface hardness and scratch resistance

PLEXIGLAS® df21 8N, PLEXIGLAS® df22 8N and PLEXIGLAS® df23 8N are special in that they combine good diffusing power with excellent light transmission.

PLEXIGLAS df molding compounds are the optimal choice, when a combination of high light scattering and excellent light transmission is required. Both, PLEXIGLAS df22 8N and PLEXIGLAS df23 8N are well designed for lamp covers, projected areas and similar applications. For displays and backlight units PLEXIGLAS df21 8N is the favored material.

Information provided by degussa.

The former Evonik Methacrylates business has been sold to Röhm GmbH (Roehm).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccISO 1183
Melt Flow 2.499 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 65.0 MPa5 mm/min; ISO 527
Elongation at Break 2.5 %5 mm/min; ISO 527
Tensile Modulus 3.30 GPa1 mm/min; ISO 527
Charpy Impact Unnotched 1.60 J/cm²
@Temperature 23.0 °C
ISO 179
 
Thermal PropertiesOriginal ValueComments
CTE, linear 63.0 µm/m-°C
@Temperature 0.000 - 50.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 103 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °CISO 75
Vicat Softening Point 109 °CB50; ISO 306
Glass Transition Temp, Tg 108 °CIEC 10006
Glow Wire Test 700 °CIEC 695-2
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 81 %Transmission Factor; DIN 5036
 
Processing PropertiesOriginal ValueComments
Processing Temperature 220 - 260 °CCylinder Temperature
Melt Temperature 220 - 260 °C
Mold Temperature 60.0 - 90.0 °C
Drying Temperature <= 95.0 °CPredrying
Dry Time 2 - 3 hourDesiccant-type drier
 
Descriptive Properties
Energy Half Angle20°IEC 695-2
Fire RatingB2DIN 4102

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röhm Plexiglas® df22 8N Molding Compound
Röhm Plexiglas® df21 8N Molding Compound
Röhm Plexiglas® 8N PMMA Molding Compound
Röhm PLEXIGLAS® Satinice df20 8N PMMA
Röhm PLEXIGLAS® Satinice df23 7N PMMA

PHUK025 / 47159

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.