MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® 1454 125°C Curing Epoxy Matrix  (discontinued **)
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: HexPly® 1454 is a self-extinguishing epoxy resin system with very high self adhesion properties. It has good handling and is tolerant of a wide range of processing conditions. HexPly® 1454 is ideal for the fabrication of honeycomb sandwich structures when high peel strength and good impact properties are required. HexPly® 1454 prepregs are only available with fabric reinforcements.

Features: Controlled flow matrix, Good tack life, Very tacky, Self extinguishing, Self adhesive on honeycomb and foam, Suitable for a range of pressure (0.8 to 5 bar), Versatile cure cycle 100-150°C, Good impact resistance

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.26 g/ccCured resin density
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 65.0 MPaISO R527 Type 1
Elongation at Yield 3.3 %ISO R527 Type 1
Tensile Modulus 3.06 GPaISO R527 Type 1
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 110 - 120 °CDMA
 
Processing PropertiesOriginal ValueComments
Shelf Life 18.0 Month
@Temperature -18.0 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexPly® 8552 Epoxy Matrix
Hexcel® HexPly® 171/174/176 120°C Curing Epoxy Matrix
Hexcel® HexPly® 6376 175°C Curing Epoxy Matrix
Hexcel® HexPly® 913 125°C Curing Epoxy Matrix
Hexcel® HexPly® 914 175°C Curing Epoxy Matrix

PHEXC040 / 98510

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.