MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Halar® 1400LC ECTFE
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; ECTFE Fluoropolymer

Material Notes: Used for fibers

Features: Low Viscosity

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.68 g/cc0.0607 lb/in³ASTM D792
Water Absorption at Saturation <= 0.10 %<= 0.10 %ASTM D570
Linear Mold Shrinkage, Flow 0.025 cm/cm0.025 in/inASTM D955
Melt Flow 500 g/10 min
@Load 2.16 kg,
Temperature 275 °C
500 g/10 min
@Load 4.76 lb,
Temperature 527 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 7373ASTM D785
Hardness, Shore D 6969ASTM D2240
Tensile Strength, Yield 30.0 MPa4350 psi50 mm/min; ASTM D638
Elongation at Yield 1.0 - 10 %1.0 - 10 %50 mm/min; ASTM D638
Tensile Modulus 1.78 GPa258 ksi50 mm/min; ASTM D638
Flexural Strength 47.0 MPa6820 psi2.5 mm/min; ASTM D790
Flexural Modulus 1.69 GPa245 ksi2.5 mm/min; ASTM D790
Izod Impact, Notched  0.190 J/cm
@Thickness 3.20 mm,
Temperature -40.0 °C
0.356 ft-lb/in
@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256
 0.250 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
0.468 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Coefficient of Friction, Dynamic 0.200.20vs. Itself; ASTM D1894
Coefficient of Friction, Static 0.200.20vs. Itself; ASTM D1894
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.50e+16 ohm-cm5.50e+16 ohm-cmASTM D257
Dielectric Constant 2.57
@Frequency 1e+6 Hz
2.57
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 14.0 kV/mm
@Thickness 3.20 mm
356 kV/in
@Thickness 0.126 in
ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 100 µm/m-°C55.6 µin/in-°FASTM D696
Specific Heat Capacity 0.962 J/g-°C0.230 BTU/lb-°FASTM C351
Thermal Conductivity 0.150 W/m-K
@Temperature 40.0 °C
1.04 BTU-in/hr-ft²-°F
@Temperature 104 °F
ASTM C177
Melting Point 235 °C455 °F
Deflection Temperature at 0.46 MPa (66 psi) 109 °C228 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C154 °FUnannealed; ASTM D648
Decomposition Temperature 300 °C572 °FTGA
Flammability, UL94 V-0V-0
Oxygen Index 52 %52 %ASTM D2863
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
FormsPellets
ProcessingMeltblown Nonwovens

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4215 / 280015

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.