MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Halar® 1400LC ECTFE
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; ECTFE Fluoropolymer

Material Notes: Used for fibers

Features: Low Viscosity

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.68 g/ccASTM D792
Water Absorption at Saturation <= 0.10 %ASTM D570
Linear Mold Shrinkage, Flow 0.025 cm/cmASTM D955
Melt Flow 500 g/10 min
@Load 2.16 kg,
Temperature 275 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 73ASTM D785
Hardness, Shore D 69ASTM D2240
Tensile Strength, Yield 30.0 MPa50 mm/min; ASTM D638
Elongation at Yield 1.0 - 10 %50 mm/min; ASTM D638
Tensile Modulus 1780 MPa50 mm/min; ASTM D638
Flexural Strength 47.0 MPa2.5 mm/min; ASTM D790
Flexural Modulus 1690 MPa2.5 mm/min; ASTM D790
Izod Impact, Notched 19.0 J/m
@Thickness 3.20 mm,
Temperature -40.0 °C
ASTM D256
 25.0 J/m
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
Coefficient of Friction, Dynamic 0.20vs. Itself; ASTM D1894
Coefficient of Friction, Static 0.20vs. Itself; ASTM D1894
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.50e+16 ohm-cmASTM D257
Dielectric Constant 2.57
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 14.0 kV/mm
@Thickness 3.20 mm
ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 100 µm/m-°CASTM D696
Specific Heat Capacity 0.962 J/g-°CASTM C351
Thermal Conductivity 0.150 W/m-K
@Temperature 40.0 °C
ASTM C177
Melting Point 235 °C
Deflection Temperature at 0.46 MPa (66 psi) 109 °CUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °CUnannealed; ASTM D648
Decomposition Temperature 300 °CTGA
Flammability, UL94 V-0
Oxygen Index 52 %ASTM D2863
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
FormsPellets
ProcessingMeltblown Nonwovens

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4215 / 280015

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.