MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® A3X2G7 BK 23187 35% Glass Filled PA66 FR (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Description: 35% glass-fiber reinforced injection-molding grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stiffness and strength; outstanding mechanical and electrical properties.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.500 - 0.800 g/cc
Density 1.45 g/ccISO 1183
Moisture Absorption at Equilibrium 1.0 - 1.4 %23°C; 50% RH; ISO 62
Water Absorption at Saturation 4.4 - 5.0 %ISO 62
Viscosity Measurement 140ISO 307
Linear Mold Shrinkage 0.0045 cm/cmrestricted
Linear Mold Shrinkage, Flow 0.0034 cm/cmISO 2577
Linear Mold Shrinkage, Transverse 0.0114 cm/cmISO 2577
Melt Flow 43.5 g/10 min
@Load 5.00 kg,
Temperature 275 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 160 MPa50 mm/min; ISO 527-1/-2
Elongation at Yield 3.0 %50 mm/min; ISO 527-1/-2
Modulus of Elasticity 11.0 GPaISO 527-1/-2
Flexural Modulus 9200 MPaISO 178
Izod Impact, Notched (ISO) 13.0 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Charpy Impact Unnotched 65.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 70.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 14.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 60093
Dielectric Constant 3.6
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VTest solution A; IEC 60112
Hot Wire Ignition, HWI 2.0 sec
@Thickness >=0.750 mm
ASTM D3874-88
High Amp Arc Ignition, HAI 0.00 arcs
@Thickness >=0.400 mm
UL 746C
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 15.0 - 20.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
DIN 11359-1/-2
CTE, linear, Transverse to Flow 60.0 - 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
DIN 11359-1/-2
Specific Heat Capacity 1.40 J/g-°C
Thermal Conductivity 0.340 W/m-KDIN 52612
Melting Point 260 °CDIN 53765
Maximum Service Temperature, Air 140 °Cfor 50% loss of tensile strength after 20000hr
 157 °Cfor 50% loss of tensile strength after 5000hr
 220 °C
Deflection Temperature at 0.46 MPa (66 psi) 250 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 250 °CISO 75-1/-2
Decomposition Temperature >= 310 °C
UL RTI, Electrical 115 °C
@Thickness 1.50 mm
UL 746B
Flammability, UL94 HB
@Thickness >=0.400 mm
 V-0
@Thickness >=0.750 mm
 5VB
@Thickness >=1.50 mm
Oxygen Index 28 %ISO 4589-2
Glow Wire Flammability Index 960 °C
@Thickness 0.800 mm
IEC 60695-2-12
Ignition Temperature >= 350 °CASTM D1929
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 °CHopper Throat
Zone 1 290 °CFeed Zone
Zone 2 290 °CCompression
Zone 3 290 °CMetering-zone
Zone 4 290 °CNozzle
Melt Temperature 280 - 300 °CInjection-molding/Extrusion
 290 °COptimal
Mold Temperature 80.0 °COptimal
 80.0 - 90.0 °CInjection-molding
Drying Temperature 80.0 °C
Dry Time 4 hour
Moisture Content 0.030 - 0.060 %Optimal
 <= 0.15 %
 
Descriptive Properties
ColorBK 23187
Commercial StatusEurope
Peripheral Screw Speed< 0.3 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® A3X2G7 BK 23187 35% Glass Filled PA66 FR (Conditioned)
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Conditioned)
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Dry)
BASF Ultramid® A3X2G5 25% Glass Filled PA66 (Dry)
BASF Ultramid® FRee A3U40G5 25% Glass Filled PA66 FR (Dry)

PBASG0312 / 131945

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.