MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Neostar FN006 Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE; Polyester, TP

Material Notes: Neostar FN006 elastomer is the second in Eastman’s series of tough, clear, durable copolyester ethers. Developed for use in the profile and automotive markets, it can also be used in packaging and tubing applications. Its chemical resistance, flexibility, and toughness make it an ideal choice for applications where strength, durability, and puncture resistance in harsh environments is required. Neostar FN006 can be used in injection molding or cast film, blown film, or tubing extrusion applications. This copolyester has a full range of flexibility and memory without the addition of plasticizers. Considered environmentally preferred due to its non-halogenated material composition, it can be incinerated cleanly without the emission of toxic gases. The target inherent viscosity of this product is 1.6.

Applications/Uses

  • Automotive
  • Flexible hinges
  • Pricing channels
  • Retail pricing fins
  • Driver and passenger side air bags
  • Packaging
  • Profiles
  • Tubing
  • Key Attributes

  • Environmentally preferred, non-halogenated material
  • Excellent chemical resistance
  • Exceptional heat resistance and high temperature dimensional stability
  • High flexibility without plasticizers
  • Solvent bondable
  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Specific Gravity 1.13 g/ccASTM D792
    Water Absorption 0.40 %24h Immersion; ASTM D570
    Viscosity Measurement 1.16Inherent; EMN-A-AC-G-V-1
    Melt Flow 10 g/10 min
    @Load 2.16 kg,
    Temperature 230 °C
    ASTM D1238
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Shore A 95ASTM D2240
    Hardness, Shore D 55ASTM D2240
    Tensile Strength at Break 22.0 MPaASTM D638
    Tensile Strength, Yield 14.0 MPaASTM D638
    Elongation at Break 400 %ASTM D638
    Elongation at Yield 38 %ASTM D638
    Tensile Modulus 0.170 GPaASTM D638
    Flexural Modulus 0.150 GPaASTM D790
    Izod Impact, Notched 0.400 J/cm
    @Temperature -40.0 °C
    ASTM D256
    Tear Strength, Total 350 NASTM D1004
     
    Thermal PropertiesOriginal ValueComments
    Heat of Fusion 27.0 J/gASTM E793
    CTE, linear 150 µm/m-°C
    @Temperature 20.0 °C
    ASTM D696
    Specific Heat Capacity 1.60 J/g-°CDSC
     1.80 J/g-°C
    @Temperature 100 °C
    DSC
     2.00 J/g-°C
    @Temperature 150 °C
    DSC
     2.30 J/g-°C
    @Temperature 175 °C
    solid; DSC
     2.30 J/g-°C
    @Temperature 225 °C
    melt; DSC
     3.10 J/g-°C
    @Temperature 200 °C
    transition; DSC
    Thermal Conductivity 0.190 W/m-KASTM C177
    Melting Point 205 °CCrystalline Peak; ASTM D3418
    Crystallization Temperature 140 °Con cooling; DSC
    Vicat Softening Point 170 °C1kg load; ASTM D1525
    Brittleness Temperature <= -75.0 °CASTM D746
    Glass Transition Temp, Tg -3.00 °CDSC
    Clash Berg Stiffness Temperature <= -70.0 °Cat 930 MPa; ASTM D1043
     -28.0 °Cat 240 MPa; ASTM D1043

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Eastman Neostar FN007 Elastomer
    Eastman Neostar FN005 Elastomer
    Dow AFFINITY™ SM 1350 Polyolefin Plastomer
    Eastman Ecdel PCCE 9967 Copolyester Ether Elastomer
    Network Polymers Softflex® 0470

    PE9090 / 35146

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.