MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Rogers Corporation Bisco® EC-2040 Conductive Silicone
Categories: Polymer; Thermoset; Silicone

Material Notes:
  • Base Polymer: Silicone
  • Filler: Nickel-Graphite
  • Applications: Silicone EMI Shields
  • Thickness: 0.020 inches and 0.031 inches

Information provided by Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.18 g/cc
Thickness 20.0 - 31.0 milRange of Thicknesses Available
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40ASTM D2240
Hardness, Shore OO 85ASTM D2240
Tensile Strength >= 90.0 psiASTM D142
Elongation at Break <= 60 %ASTM D412
Compression Set 3.0 %
@Temperature 70.0 °C
% of thickness; ASTM D3574
 6.0 %
@Temperature 100 °C
% of thickness; ASTM D395 Method B
 12 %
@Temperature 70.0 °C
% of deflection; ASTM D3574
 22 %
@Temperature 100 °C
% of deflection; ASTM D395 Method B
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.20 ohm-cmRogers Corp. Internal
Shielding Effectiveness 85 dB
@Thickness 0.508 mm,
Frequency 1e+10 Hz
MIL G83528
 110 dB
@Thickness 0.508 mm,
Frequency 1e+9 Hz
MIL G83528
 120 dB
@Thickness 0.508 mm,
Frequency 1e+8 Hz
MIL G83528
 120 dB
@Thickness 0.508 mm,
Frequency 5.00e+8 Hz
MIL G83528

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Precision Polymer Engineering S70L Conductive Silicone Rubber
Aluminum 2124-T351
Overview of materials for Silicone Rubber
Shin-Etsu Silicones X-65-130U Electrically Conductive Silicone Elastomer
Silicon, Si

PROGA910 / 138350

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.