MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Elite® 5200 Linear Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: ELITE® 5200 enhanced polyethylene resin is a copolymer produced via INSITE® Technology from Dow Plastics. This resin offers high impact strength and good puncture resistance at moderate stretch levels for irregularly shaped loads. In addition, ELITE 5200 resin provides excellent on-pallet elongation for higher yields on regular loads. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2 (a) when used unmodified and processed according to good manufacturing practices.

Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.917 g/cc
Melt Flow 4.0 g/10 min
@Load 2.16 kg
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 10.3 MPa
Film Tensile Strength at Yield, TD 8.80 MPa
Film Elongation at Break, MD 460 %
Film Elongation at Break, TD 620 %
Elmendorf Tear Strength MD 320 gUnspecified film thickness
Elmendorf Tear Strength TD 460 gUnspecified film thickness
Dart Drop Test 300 g
Film Tensile Strength at Break, MD 38.6 MPa
Film Tensile Strength at Break, TD 29.7 MPa
 
Optical PropertiesOriginal ValueComments
Haze 0.80 %
Gloss 95 %45°
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow HDPE 10462N High Density Polyethylene
Huntsman PE5080 Extrusion Coating Polyethylene
Dow ELITE™ 5500G Enhanced Polyethylene Resin
Dow ELITE™ 5401G Enhanced Polyethylene Resin
Dow ELITE™ 5400G Enhanced Polyethylene Resin

PDW471 / 34540

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.