MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Network Polymers SAN 290 High Flow Natural
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Transparent

Material Notes: Description: SAN - Styrene Acrylonitrile Transparent Engineering Thermoplastic

Information provided by Network Polymers Inc.

A. Schulman has acquired Network Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/ccASTM D792
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cmASTM D955
Melt Flow 8.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
Procedure A Condition G; ASTM D1238
 31.1 g/10 min
@Load 3.80 kg,
Temperature 230 °C
Procedure A Condition I; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 70ASTM D785
Tensile Strength, Yield 10000 psichs 2 in/min; ASTM D638
Flexural Modulus 500000 psiTangent, chs 0.05 in/min; ASTM D790
Izod Impact, Notched 0.400 ft-lb/in0.125 inch bar; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 196 °FUnannealed/Conditioned 48 hours at 23°C; ASTM D648
Vicat Softening Point 100 °C0.125 inch bar, 1 Kg; ASTM D1525
Flammability, UL94 HB
@Thickness 1.59 mm
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema OREVAC® 18910 Maleic Anhydride Modified Copolymer
Americhem Engineered Compounds ColorFast® JCT1000 Polycarbonate-ABS-SMA Alloy
INEOS Styrolution PS 3190/3191 GPPS
INEOS Styrolution PS 3100/3101 GPPS
INEOS Styrolution PS 1900 GPPS

PDIAM035 / 29873

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.