MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
3M Novec™ 72DE Engineered Fluid
Categories: Fluid

Material Notes: 3M™ Novec™ 72DE is intended for heavy duty cleaning and degreasing applications. The high solvency and low toxicity make it an ideal replacement for ozone-depleting compounds, chlorinated solvents, and n-propyl bromide in many applications

Feature and Benefits:

  • Non-flammable
  • Non-conductive
  • Low toxicity
  • Low Global Warming Potential (GWP)
  • Zero ozone depletion potential
  • Low surface tension penetrates tight spaces for improved cleaning

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.28 g/ccLiquid
Viscosity 0.45 cP
Vapor Pressure 0.467 bar
Surface Tension 19 dynes/cm
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 217.7 J/g
Boiling Point 43.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Novec™ 7100DL Engineered Fluid
3M Novec™ 7100 Engineered Fluid
3M Novec™ 7000 Engineered Fluid
3M Novec™ 649 Engineered Fluid
3M Novec™ 71DA Engineered Fluid

PMM33112 / 167859

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.