MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Rogers Arlon Secure™ 48A50B020 0.020" Thermally Conductive Silicone Rubber Adhesive on Fiberglass for Solar Cell Encapsulation
Categories: Polymer; Thermoset; Silicone; Silicone, Molded, Glass Fiber Filled

Material Notes: Secure™ Thermally Conductive Silicone Rubber Adhesive on Fiberglass for Solar Cell Encapsulation

Design/Construction:

  • Liner: 2.5 mil Polyethylene
  • Side 1: Uncured Rubber
  • Substrate: 1080 Style Fiberglass

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.80 g/cc0.101 lb/in³Silicone Property; Arlon SQA-TMS-024
Thickness 76.2 microns3.00 milSubstrate; Arlon SQA-TMS-003
 432 microns17.0 milSilicone; Arlon SQA-TMS-003
 508 microns20.0 milOverall Thickness; Arlon SQA-TMS-003
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7777Silicone Property; ASTM D2240
Tensile Strength 4.72 MPa685 psiSilicone Property; ASTM D412
Tensile Strength, Yield 24.5 MPa
@Strain <=1 %
3550 psi
@Strain <=1 %
Silicone Property; Arlon SQA-TMS-008
Elongation at Break 125 %125 %Silicone Property; ASTM D412
Poissons Ratio 0.500.50
Peel Strength 0.351 kN/m2.00 pliBond Strength (S1 to S1); Arlon SQA-TMS-024
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 6.9
@Frequency 1e+6 Hz
6.9
@Frequency 1e+6 Hz
Silicone Property; IPC TM 6550 - 2.5.5.3
Dielectric Strength 31.9 kV/mm810 kV/inASTM D149
Dissipation Factor 0.0044
@Frequency 1e+6 Hz
0.0044
@Frequency 1e+6 Hz
Silicone Property; IPC TM 6550 - 2.5.5.3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 105 µm/m-°C
@Temperature 20.0 - 160 °C
58.3 µin/in-°F
@Temperature 68.0 - 320 °F
Silicone Property; ASTM E831
Specific Heat Capacity 0.820 J/g-°C
@Temperature 100 °C
0.196 BTU/lb-°F
@Temperature 212 °F
Silicone Property; Arlon SQA-TMS-052
Thermal Conductivity 1.40 W/m-K
@Temperature 100 °C
9.72 BTU-in/hr-ft²-°F
@Temperature 212 °F
Silicone Property; ASTM E1530
Maximum Service Temperature, Inert 204 °C399 °F
Minimum Service Temperature, Air -100 °C-148 °F
Glass Transition Temp, Tg -118 °C-180 °FSilicone Property; ASTM D3418
UL RTI, Electrical 150 °C302 °F
UL RTI, Mechanical without Impact 150 °C302 °F
Flammability, UL94 V-0V-0E54153
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month
@Temperature 7.22 °C
3.00 Month
@Temperature 45.0 °F
 
Descriptive Properties
ColorGraySilicone
 WhiteSubstrate
Plasticity (mm)2.3Arlon SQA-TMS-005; Silicone Property

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond EP45HTQ Quartz Filled Heat Resistant Epoxy
Master Bond EP30QF Quartz filled, Two Part Epoxy System
Dymax 4-425 Glass Bonding Adhesive
Dow 733 GLASS & METAL SEALANT
APCM DA 4518U/E-Glass Unidirectional E-Glass Epoxy Prepreg

PARL9756 / 148909

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.