MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Rogers Arlon Secure™ 48A50B020 0.020" Thermally Conductive Silicone Rubber Adhesive on Fiberglass for Solar Cell Encapsulation
Categories: Polymer; Thermoset; Silicone; Silicone, Molded, Glass Fiber Filled

Material Notes: Secure™ Thermally Conductive Silicone Rubber Adhesive on Fiberglass for Solar Cell Encapsulation

Design/Construction:

  • Liner: 2.5 mil Polyethylene
  • Side 1: Uncured Rubber
  • Substrate: 1080 Style Fiberglass

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.80 g/ccSilicone Property; Arlon SQA-TMS-024
Thickness 3.00 milSubstrate; Arlon SQA-TMS-003
 17.0 milSilicone; Arlon SQA-TMS-003
 20.0 milOverall Thickness; Arlon SQA-TMS-003
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 77Silicone Property; ASTM D2240
Tensile Strength 685 psiSilicone Property; ASTM D412
Tensile Strength, Yield 3.55 ksi
@Strain <=1 %
Silicone Property; Arlon SQA-TMS-008
Elongation at Break 125 %Silicone Property; ASTM D412
Poissons Ratio 0.50
Peel Strength 2.00 pliBond Strength (S1 to S1); Arlon SQA-TMS-024
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 6.9
@Frequency 1e+6 Hz
Silicone Property; IPC TM 6550 - 2.5.5.3
Dielectric Strength 810 V/milASTM D149
Dissipation Factor 0.0044
@Frequency 1e+6 Hz
Silicone Property; IPC TM 6550 - 2.5.5.3
 
Thermal PropertiesOriginal ValueComments
CTE, linear 105 µm/m-°C
@Temperature 20.0 - 160 °C
Silicone Property; ASTM E831
Specific Heat Capacity 0.820 J/g-°C
@Temperature 100 °C
Silicone Property; Arlon SQA-TMS-052
Thermal Conductivity 1.40 W/m-K
@Temperature 100 °C
Silicone Property; ASTM E1530
Maximum Service Temperature, Inert 399 °F
Minimum Service Temperature, Air -148 °F
Glass Transition Temp, Tg -118 °CSilicone Property; ASTM D3418
UL RTI, Electrical 302 °F
UL RTI, Mechanical without Impact 302 °F
Flammability, UL94 V-0E54153
 
Processing PropertiesOriginal ValueComments
Shelf Life 3.00 Month
@Temperature 7.22 °C
 
Descriptive Properties
ColorGraySilicone
 WhiteSubstrate
Plasticity (mm)2.3Arlon SQA-TMS-005; Silicone Property

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP45HTQ Quartz Filled Heat Resistant Epoxy
Master Bond EP30QF Quartz filled, Two Part Epoxy System
Dymax 4-425 Glass Bonding Adhesive
Dow 733 GLASS & METAL SEALANT
APCM DA 4518U/E-Glass Unidirectional E-Glass Epoxy Prepreg

PARL9756 / 148909

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.