MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Crucible Steel CPM® REX® 121 HS High Speed Steel
Categories: Metal; Ferrous Metal; Tool Steel

Material Notes: CPM REX 121 is a new high vanadium cobalt bearing tool steel designed to offer a combination of the highest wear resistance, attainable hardness, and red hardness available in a high speed steel. Its superior red hardness permits higher cutting speeds compared to other high speed steels. Its superior wear resistance (due to the high vanadium content) helps maintain a sharp cutting edge at increased cutting speeds.

CPM REX 121 also bridges the performance gap between high alloy tool steels and carbide materials. It may be used in cutting tools, where high cutting speeds demand higher heat resistance, but carbide is too brittle, or in high wear tooling applications (punches and dies) where carbide tools are too fragile.

Because of the extremely fine and uniform CPM microstructure, sulfur may be added if desired, to improve the machinability. The higher sulfur content benefits the toolmaker by allowing ease of manufacture, and the tool user by allowing easier resharpening. The CPM process ensures that the additional sulfur will not detrimentally affect the tool’s toughness.

Information provided by Crucible Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 360 - 410
Hardness, Rockwell C 71hardened at 1875°F
 55
@Tempering Temp. 649 °C
hardened at 1875°F then tempered
 63
@Tempering Temp. 593 °C
hardened at 1875°F then tempered
 66.5
@Tempering Temp. 566 °C
hardened at 1875°F then tempered
 67.5
@Tempering Temp. 551.7 °C
hardened at 1875°F then tempered
 68.5
@Tempering Temp. 538 °C
hardened at 1875°F then tempered
 69
@Tempering Temp. 510 °C
hardened at 1875°F then tempered
Modulus of Elasticity 31000 ksi
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 3.4 %
Chromium, Cr 4.0 %
Cobalt, Co 9.0 %
Iron, Fe 59 %as balance
Molybdenum, Mo 5.0 %
Sulfur, S 0.030 %
Tungsten, W 10 %
Vanadium, V 9.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Assab Steels ASP 60 Cold Work Steel
AISI Grade 18Ni (250) Maraging Steel, Aged, 6 mm sheet, tested transverse
AISI 1015 Steel, cold drawn
Bohler-Uddeholm UDDEHOLM VANADIS 60 Powder Metallurgically Produced Tool Steel
Overview of materials for AISI 1000 Series Steel

NCRUC932 / 160383

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.