MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Special Metals NILO® 365 Controlled-Expansion Alloy  (discontinued **)
Categories: Metal; Ferrous Metal; Superalloy; Iron Base

Material Notes: For the manufacture of tooling for composites, the NILO® nickel-iron alloys offer a unique combination of matched thermal expansion to avoid warping during the curing cycle, along with strength, rigidity, durability, ease of fabrication and availability.

NILO alloy 365 has 43% nickel and is strengthened by additions of 1.4% Ti and 3.3% Nb. Strengthening occurs during the aging heat-treatment – 1250°F (677°C) for 4 hours, furnace cool at 100°F (38°C) per hour to 1150°F (621°C) for 4 hours, air cool – producing a gamma prime precipitate. Agehardened NILO alloy 365 develops higher room-temperature hardness (Rockwell C39) and four times the yield strength – 146 ksi (1006 MPa) – compared with annealed 36% Ni-Fe alloys. Creep strength (resistance to deformation under load) is also much higher.

Information Provided by Special Metals Corporation

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.11 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 717 MPaAnnealed
 1269 MPaAnnealed and Age Hardened
Tensile Strength, Yield 407 MPa
@Strain 0.2 %
Annealed
 1007 MPa
@Strain 0.2 %
Annealed and Age Hardened
Elongation at Break 16 %50 mm, Annealed and Age Hardened
 41 %50 mm, Annealed
Reduction of Area 36 %Annealed and Age Hardened
 63 %Annealed
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.500 J/g-°C
Thermal Conductivity 12.4 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.020 %
Iron, Fe 51.78 %Balance
Nickel, Ni 43.5 %
Niobium, Nb (Columbium, Cb) 3.3 %
Titanium, Ti 1.4 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals NILO® Alloy 42 Controlled-Expansion Alloy
Special Metals NILO® Alloy 48 Controlled-Expansion Alloy
Aperam FeNi 70 Controlled Expansion Alloys Iron-Nickel Alloys
Ductile Iron grade 80-55-06
Special Metals INCOLOY® Alloy 330

NINDA23 / 98914

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.