MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Special Metals NILO® Alloy 48 Controlled-Expansion Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy; Iron Base

Material Notes: Inflection point 460°C. A nickel-iron controlled-expansion alloy containing 48% nickel. Its coefficient of thermal expansion is designed to match that of soft lead and soda-lime glasses. The alloy also has a high inflection point. Used for glass-to-metal seals in radio valves and incandescent electric light bulbs and for industrial thermostats that operate at temperatures up to 840°F (450°C). Standard product forms are round, flats, tube, strip, and wire.

Data provided by the manufacturer, Special Metals.

Key Words: UNS K94800; ASTM F 30; DIN 17745; Werkstoff Nr. 1.3922, 1.3926, 1.3927; AFNOR NF A54-301
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.20 g/cc0.296 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 520 MPa75400 psiAnnealed prior to test
 470 MPa
@Temperature 300 °C
68200 psi
@Temperature 572 °F
Annealed prior to test
Tensile Strength, Yield 260 MPa
@Strain 0.2 %
37700 psi
@Strain 0.2 %
Annealed prior to test
 160 MPa
@Strain 0.2 %,
Temperature 300 °C
23200 psi
@Strain 0.2 %,
Temperature 572 °F
Annealed prior to test
Elongation at Break 42 %42 %Annealed prior to test.
 43 %
@Temperature 300 °C
43 %
@Temperature 572 °F
Annealed prior to test.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000470 ohm-cm0.0000470 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  8.50 µm/m-°C
@Temperature 20.0 - 100 °C
4.72 µin/in-°F
@Temperature 68.0 - 212 °F
 8.30 - 9.30 µm/m-°C
@Temperature 20.0 - 400 °C
4.61 - 5.17 µin/in-°F
@Temperature 68.0 - 752 °F
Thermal Conductivity 16.7 W/m-K116 BTU-in/hr-ft²-°F
Melting Point 1450 °C2640 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.10 %<= 0.10 %
Carbon, C <= 0.050 %<= 0.050 %
Chromium, Cr <= 0.25 %<= 0.25 %
Cobalt, Co <= 1.0 %<= 1.0 %
Iron, Fe 49 %49 %As remainder
Manganese, Mn <= 0.80 %<= 0.80 %
Nickel, Ni 48 %48 %nominal; adjustable to meet expansion requirements
Phosphorus, P <= 0.025 %<= 0.025 %
Silicon, Si <= 0.30 %<= 0.30 %
Sulfur, S <= 0.025 %<= 0.025 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals NILO® Alloy 42 Controlled-Expansion Alloy
California Fine Wire Alloy 52 Nickel Iron Alloy
Aperam FeNi 70 Controlled Expansion Alloys Iron-Nickel Alloys
Carpenter Invar 36® Alloy, Cold Drawn Bars
Nickel Iron Alloy 52 Sealing Wire, UNS N14052

NIND22 / 17526

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.