MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® A 218HP V35 PA66, 35% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Description: TECHNYL® A 218HP V35 is a polyamide 6.6, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in black color.

Benefits: The product offers an outstanding long term heat resistance and is suitable to work in environments characterized by a very high temperature.

Available in: Asia Pacific, Europe and Latin America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

Applications: It is used in a wide variety of industries, especially in automotive industry for air circuit parts such as intercoolers.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³ISO 1183/A
Linear Mold Shrinkage 0.0077 cm/cm0.0077 in/inIsotropy
Linear Mold Shrinkage, Flow 0.0046 cm/cm0.0046 in/in
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 170 MPa24700 psiISO 527 Type 1A
Tensile Stress at Strain  35.0 MPa
@Strain 1 %,
Temperature 200 °C
5080 psi
@Strain 1 %,
Temperature 392 °F
 45.0 MPa
@Strain 3 %,
Temperature 200 °C
6530 psi
@Strain 3 %,
Temperature 392 °F
 50.0 MPa
@Strain 4 %,
Temperature 200 °C
7250 psi
@Strain 4 %,
Temperature 392 °F
 100 MPa
@Strain 1 %,
Temperature 23.0 °C
14500 psi
@Strain 1 %,
Temperature 73.4 °F
 180 MPa
@Strain 2 %,
Temperature 23.0 °C
26100 psi
@Strain 2 %,
Temperature 73.4 °F
 400 MPa
@Strain 2 %,
Temperature 200 °C
58000 psi
@Strain 2 %,
Temperature 392 °F
Elongation at Break 2.8 %2.8 %ISO 527 Type 1A
Tensile Modulus 10.7 GPa1550 ksiISO 527 Type 1A
Flexural Strength 250 MPa36300 psiISO 178
Flexural Modulus 8.70 GPa1260 ksiISO 178
Charpy Impact Unnotched 7.50 J/cm²35.7 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.30 J/cm²6.19 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 247 °C477 °FISO 75/Af
 
Processing PropertiesMetricEnglishComments
Feed Temperature 260 - 270 °C500 - 518 °F
Front Barrel Temperature 280 - 290 °C536 - 554 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.12 %<= 0.12 %
 
Descriptive Properties
Compression Zone270-280°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, DRY
Domo TECHNYL® A 218 PA66, 33% glass fiber, DRY
Domo TECHNYL® A 218G V30 PA66, 30% glass fiber, DRY
Domo TECHNYL® A 218G2 V30 Black 34N PA66, 30% glass fiber, DRY
Domo Technyl® C216V30 30% Glass Filled Nylon 6

PRHOD672 / 137903

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.