MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Epoxies, Etc 20-1625 Optically Clear Silicone Potting and Encapsulating Compound
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: 20-1625 is a low viscosity and easy to use 1:1 ratio silicone system. It is designed for applications that require clarity and protection from shock and vibration. 20-1625 provides good heat resistance and is flame retardant. 20-1625 is formulated without solvents or other toxic materials. It is therefore not regulated or considered hazardous for transportation.

Features:

  • Easy 1:1 mix ratio
  • Soft
  • Excellent electrical properties
  • Solvent free
  • Optically clear
Benefits:
  • Simple to use
  • Low stress on components and vibration resistant
  • Extends life of electronic assemblies
  • No by-products released during cure and safe to handle
  • Easy component identification

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.980 g/cc0.980 g/ccResin (Part A)
 0.980 g/cc0.980 g/ccActivator (Part B)
Viscosity 4000 cP4000 cPActivator (Part B)
 4500 cP4500 cPResin (Part A)
Storage Temperature 18.0 - 27.0 °C64.4 - 80.6 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2525
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cm
Dielectric Constant 2.7
@Frequency 60 Hz
2.7
@Frequency 60 Hz
Dielectric Strength 19.7 kV/mm500 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 270 µm/m-°C150 µin/in-°F
Thermal Conductivity 0.159 W/m-K1.10 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 20.0 °C68.0 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 min
@Temperature 60.0 °C
1.00 hour
@Temperature 140 °F
 180 - 240 min
@Temperature 25.0 °C
3.00 - 4.00 hour
@Temperature 77.0 °F
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
ColorClearResin (Part A)
 ClearActivator (Part B)
Working Time20 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFEPOX001 / 316678

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.