MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Epoxies, Etc 20-1625 Optically Clear Silicone Potting and Encapsulating Compound
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: 20-1625 is a low viscosity and easy to use 1:1 ratio silicone system. It is designed for applications that require clarity and protection from shock and vibration. 20-1625 provides good heat resistance and is flame retardant. 20-1625 is formulated without solvents or other toxic materials. It is therefore not regulated or considered hazardous for transportation.

Features:

  • Easy 1:1 mix ratio
  • Soft
  • Excellent electrical properties
  • Solvent free
  • Optically clear
Benefits:
  • Simple to use
  • Low stress on components and vibration resistant
  • Extends life of electronic assemblies
  • No by-products released during cure and safe to handle
  • Easy component identification

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.980 g/ccResin (Part A)
 0.980 g/ccActivator (Part B)
Viscosity 4000 cPActivator (Part B)
 4500 cPResin (Part A)
Storage Temperature 18.0 - 27.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 25
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cm
Dielectric Constant 2.7
@Frequency 60 Hz
Dielectric Strength 500 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 270 µm/m-°C
Thermal Conductivity 1.10 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 20.0 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 - 4.00 hour
@Temperature 25.0 °C
 60.0 min
@Temperature 60.0 °C
Shelf Life 6.00 Month
 
Descriptive Properties
ColorClearResin (Part A)
 ClearActivator (Part B)
Working Time20 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PFEPOX001 / 316678

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.