MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil HD 5402 High Density Polyethylene Copolymer Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: ExxonMobil™ HD 5402 is a pipe extrusion grade high density polyethylene copolymer offering an excellent combination of stiffness and stress crack resistance. This material meets or exceeds the AASHTO M294

Availability: Latin America, North America and South America

Additive:

  • Thermal Stabilizer: Yes
  • Antistatic: No
Applications:
  • Agriculture Products Containers
  • Caps and Closures
  • Food packaging
  • Highway Drainage Pip
  • Household and Industrial chemical containers
  • Thermoformed Parts
  • Thin Gauge Sheet

Information provided by ExxonMobil

Key Words: HDPE HD 7800P
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.953 g/ccExxonMobil method
Melt Flow 0.25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 30 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4100 psiASTM D638
Flexural Modulus, 1% Secant 140000 psiASTM D790
 
Descriptive Properties
Notched Constant Ligament Stress (NCLS)ASTM F2136

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Alathon 8005M-3 High Denisty Polyethylene
Ineos A4040 HDPE
ExxonMobil Paxon™ BA46-055 Blow Molding Resin
ExxonMobil Paxon™ AA53-003 Pipe Extrusion Resin
ExxonMobil HD 6605.29 Injection Molding Resin

PEX99305 / 175541

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.