MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultraform® S 1320 0021 UNC POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Ultraform S1320 0021 UNC is an easy flowing, rapidly freezing injection molding POM grade with enhanced stiffness and heat distortion resistance. It is highly stabilized to resist aggressive fuels, including hot diesel fuel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³ISO 1183
Water Absorption 0.80 %0.80 %ISO 62
Moisture Absorption at Equilibrium 0.20 %0.20 %23°C/50% R.H.; ISO 62
Melt Flow 12.9 g/10 min
@Load 2.16 kg,
Temperature 190 °C
12.9 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 155 MPa22500 psiISO 2039
Tensile Strength  6.37 MPa
@Time 2.59e+6 sec
925 psi
@Time 720 hour
Storage in biodiesel DIN 14214 at +140°C
 6.37 MPa
@Time 1.04e+7 sec
925 psi
@Time 2880 hour
Storage in biodiesel DIN 14214 at +140°C
 6.37 MPa
@Time 1.81e+7 sec
925 psi
@Time 5040 hour
Storage in biodiesel DIN 14214 at +140°C
Tensile Strength, Yield 66.0 MPa9570 psi50mm/min; ISO 527
Elongation at Break 30 %30 %ISO 527
Elongation at Yield 9.0 %9.0 %ISO 527
Modulus of Elasticity 3.00 GPa435 ksiISO 527
Izod Impact, Notched (ISO) 5.50 kJ/m²2.62 ft-lb/in²ISO 2039
Charpy Impact Unnotched 17.0 J/cm²80.9 ft-lb/in²ISO 179
 17.0 J/cm²
@Temperature -30.0 °C
80.9 ft-lb/in²
@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 0.550 J/cm²2.62 ft-lb/in²ISO 179
 0.550 J/cm²
@Temperature -30.0 °C
2.62 ft-lb/in²
@Temperature -22.0 °F
ISO 179
Tensile Creep Modulus, 1000 hours 1450 MPa210000 psiISO 899
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Constant  3.7
@Frequency 100 Hz
3.7
@Frequency 100 Hz
IEC 60250
 3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 40.0 kV/mm1020 kV/inIEC 60243-1
Dissipation Factor  0.0020
@Frequency 100 Hz
0.0020
@Frequency 100 Hz
IEC 60250
 0.0050
@Frequency 1e+6 Hz
0.0050
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VTest Solution A; IEC 60112
 600 V600 VTest Solution B; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 171 °C340 °FDIN 53765
Maximum Service Temperature, Air 100 °C212 °F
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °FISO 75
Vicat Softening Point 150 °C302 °F(50 °C/h / 50N) - B/50; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 230 °C374 - 446 °F
Mold Temperature 60.0 - 120 °C140 - 248 °F
 
Descriptive Properties
ColorNatural
Commercial StatusNorth America and Europe
Impact ModifiedNo
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Hostaform® C 13031 XF POM, Specialty
BASF Ultraform® N2320 006 POM
BASF Ultraform® S2320 003 POM
BASF Ultraform® S2320 0035 POM
BASF Ultraform® W2320 0035 POM

PBASF9110 / 84874

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.