MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Tabriz SV-0157 Extrusion Grade ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: SV0157 is one of the styrenic terpolymer (ABS) grade with improved toughness versus HIPS grades. SV0157 exhibits low shrinkage, and good dimensional stability.SV0157 has high melt strength, so is widely used for the production of extruded sheet and some of considerable size and thickness shaped. Applications: include panels for large appliances and thermoformed items such as hot tubs, recreational vehicle parts and refrigerator liner. use this information as a guide to aid you in selecting the proper resin for your application. Drying: Drying prior to processing is recommended in a desiccant dehumidifying hopper dryer. An inlet air dew point of -20°F (-29°C) or below is recommended to achieve a moisture content 0.1%. Typical drying conditions are 2 hours at 180° - 190°F (82° - 88°C). Drying for 4 hours at 160° - 170°F (71°-77°C) is also adequate.

Information provided by Tabriz Petrochemical Commercial Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.600 g/cc
Melt Flow 0.50 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D-1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 104ASTM D785
Tensile Strength, Yield 430 kg(f)/cm²ASTM D638
Flexural Yield Strength >= 580 kg(f)/cm²ASTM D790
Flexural Modulus >= 1.863 GPaASTM D790
Izod Impact, Notched (ISO) 31.0 kJ/m²ASTM D256
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 101 °C
@Load 5.10 kg
ASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tabriz 5211 EA HDPE
Tabriz HS321 Performance Expandable Polystyrene
Tabriz SD-0150 General Purpose ABS
Iran Petrochemical (PCC) SV-0157 Acrylonitrile Butadiene Styrene
Lotte Advanced Materials Starex® SV-0157 ABS, Unreinforced Extrusion Grade

PIPC101 / 48329

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.