MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Chemlon® MDM54 Nylon 6, Dry, Mineral Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Mineral Filled

Material Notes: Notes: MDM54 is a UL recognized, V-2 rated halogen & phosphorus free flame retarded, mineral filed injection molding grade of nylon 6, primarily intended for electrical applications.

Availability: Europe; North America

Fillers/Reinforcement: Mineral

Features: Flame Retardant; Good Colorability; Halogen Free; Low (to None) Phosphorus Content

Uses: Electrical/Electronic Applications

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.29 g/ccISO 1183
Moisture Absorption at Equilibrium 1.2 %50% RH; ISO 62
Linear Mold Shrinkage 0.0090 - 0.016 in/in
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 11200 psiISO 527-2
Elongation at Break 5.0 %ISO 527-2
Tensile Modulus 209000 psiISO 527-2
Flexural Yield Strength 16000 psiISO 178
Flexural Modulus 580000 psiISO 178
Izod Impact, Notched (ISO) 2.90 ft-lb/in²ISO 180
Charpy Impact, Notched 2.60 ft-lb/in²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohmIEC 60093
Dielectric Constant 3.9
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 280 V/mil
@Thickness 3.00 mm
IEC 60243-1
Dissipation Factor 0.020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index >= 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 172 °FUnannealed; ISO 72-2/A
Flammability, UL94 V-2
@Thickness 1.52 mm
Oxygen Index 24 %ISO 4589-2
Glow Wire Flammability Index 1760 °FIEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 464 - 500 °F
Middle Barrel Temperature 464 - 500 °F
Front Barrel Temperature 464 - 500 °F
Melt Temperature <= 572 °F
Mold Temperature 140 - 176 °F
Drying Temperature 176 °F
Dry Time 2.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0602 / 237093

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.