MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® Seal-Fit PA6/66 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, Unreinforced

Material Notes: Description: Transparent, tough, amorphous copolyamide for injection molding, specially developed for tight overmoulding of metal inlays.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.500 - 0.800 g/cc
Density 1.10 g/ccISO 1183
Moisture Absorption at Equilibrium 4.5 - 5.0 %ISO 62
Viscosity Measurement 125ISO 307
Linear Mold Shrinkage, Flow 0.0030 cm/cmISO 2577
Linear Mold Shrinkage, Transverse 0.0030 cm/cmISO 2577
Melt Flow 82.5 g/10 min
@Load 10.0 kg,
Temperature 230 °C
ISO 1133
 132 g/10 min
@Load 5.00 kg,
Temperature 275 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85ISO 868
Elongation at Yield 5.0 %50mm/min; ISO 527-1/-2
Tensile Modulus 2500 MPaISO 527-1/-2
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 80.0 - 120 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 - 120 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 57.0 °CISO 75-1/-2
Vicat Softening Point 68.0 °C
@Load 5.10 kg
ISO 306
Decomposition Temperature >= 300 °C
Flammability, UL94 HB
@Thickness 1.60 mm
 V-2
@Thickness 3.20 mm
Ignition Temperature >= 400 °CASTM D1929
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified
 
Processing PropertiesOriginal ValueComments
Processing Temperature 30.0 °CHopper Throat
Zone 1 200 °CFeed Zone
Zone 2 240 °CCompression
Zone 3 240 °CMetering-zone
Zone 4 240 °CNozzle
Melt Temperature 240 °COptimal
 230 - 260 °CInjection-molding/Extrusion
Mold Temperature 20.0 - 50.0 °CInjection-molding
 40.0 °COptimal
Drying Temperature 60.0 °C
Dry Time 8 hour
Moisture Content 0.030 - 0.060 %Optimal
 <= 0.15 %
 
Descriptive Properties
Commercial StatusEurope
Peripheral Screw Speed< 0.3 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® TR 90 PAMACM12
Arkema Rilsan® Clear G170 Polyamide
AlphaGary PVC 2235RSM-100 CLEAR 000X Polyvinyl Chloride Thermoplastic
Azoty Tarnow™ Tarnamid® T-27 MTR Polyamide 6 - Transparent
Dow AFFINITY™ SM 1300 Polyolefin Plastomer

PBASG0411 / 132044

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.