MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zeus FEP Tubing and Drawn Fiber
Categories: Polymer; Thermoplastic; Fluoropolymer; Fluorinated Ethylene Propylene (FEP); Fluorinated Ethylene Propylene (FEP), Molded/Extruded

Material Notes: FEP, fluorinated ethylene propylene, is a melt processable fluoropolymer that allows for long, continuous lengths and has several distinct advantages over PTFE. Applications where FEP tubing is usually chosen require more optical clarity and flexibility. In heat shrinkable form, FEP has a lower recovery temperature than PTFE. This fluoropolymer makes heat shrink and convoluted products that meet 23053/11 and 81914 Mil Spec certifications, respectively. The material has low gas and permeability properties; possesses an excellent UV transmission rating; Biocompatible –USP Class VI approved; and is Gamma sterilizable.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.12 - 2.17 g/ccASTM D792
Water Absorption 0.0040 %ASTM D257
Crystallinity 70 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 55 - 65ASTM D2240
Tensile Strength, Ultimate 18.0 - 34.0 MPaASTM D638
Elongation at Break 245 - 400 %ASTM D638
Modulus of Elasticity 0.440 - 0.640 GPaASTM D638
Flexural Modulus 0.580 - 0.620 GPaASTM D790
Coefficient of Friction 0.040 - 0.20
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 - 1.00e+18 ohm-cmASTM D257
Dielectric Constant 2.0 - 2.1
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 500 - 2000 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 100 - 135 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Thermal Conductivity 0.190 - 0.250 W/m-KASTM C177
Melting Point 265 - 275 °C
Maximum Service Temperature, Air 200 - 205 °C
Minimum Service Temperature, Air -240 - -200 °C
Glass Transition Temp, Tg 80.0 °C
Decomposition Temperature 380 - 430 °CASTM E1131
Flammability, UL94 V-0
Oxygen Index >= 95 %ASTM D2863
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.33 - 1.35
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Descriptive Properties
Radiation Resistance (MRad)10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cossa Polimeri ESTADIENE 2506 Acrylonitrile Butadiene Styrene
Zeus PFA Tubing and Drawn Fiber
Samyang Trirex® 3026PJ Polycarbonate
Zeus PVDF Tubing and Drawn Fiber
Baystar™ 7195 High Density Polyethylene, Specialty Extrusion Resin

PZEUS992 / 178057

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.