MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kareline Oy PPMS5050 Natural Fiber Reinforced Polypropylene for injection molding
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Natural fiber reinforced thermoplastic composite for injection molding. Fiber ECF bleached softwood pulp. Matrix plastic polypropylen.

Information provided by Kareline Oy Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccISO 1183
Melt Flow 5.17 g/10 minISO 1133, 200°C/10kg
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 57.0 MPaISO 527-1
Elongation at Break 4.3 %ISO 527-1
Flexural Modulus 4.20 GPaISO 178
Charpy Impact, Notched 0.300 J/cm²ISO 179
 
Processing PropertiesOriginal ValueComments
Mold Temperature 50.0 - 70.0 °C
Drying Temperature 80.0 °C10 hour, dehumidifying dryer
 100 °C4 hour, dehumidifying dryer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman Tritan™ TX1001 Copolyester
Eastman Eastar K3000 PETG Copolyester
Covestro Baypreg® F Polyurethane, Natural Fiber Glass
Covestro Baypreg® F Polyurethane, Mat Reinforced Sandwich
Borealis Bormed™ HD850MO Polypropylene Copolymer for Healthcare Applications

PKARE00 / 48692

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.