MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper Nickel, UNS C71640 Copper Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: This alloy is similar to the more common C71500, with higher strength and improved corrosion resistance. Common applications include heat exchangers and condensers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.320 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 63000 psiAnnealed
 81000 psiHard Drawn (H80 - for Tubing) or Rolled (H04 for Flat Products)
 >= 81000 psiPer ASTM B111
Tensile Strength, Yield 25000 psiAnnealed
 58000 psiHard Drawn (H80 - for Tubing) or Rolled (H04 for Flat Products)
 >= 58000 psi
@Strain 0.5 %
Per ASTM B111
Elongation at Break 4.0 %Hard Drawn (H80 - for Tubing) or Rolled (H04 for Flat Products)
 40 %Annealed
Tensile Modulus 2.20e+7 psi(C71500 Annealed)
Poissons Ratio 0.325(C71500 Annealed)
Machinability 20 %Based on Free cutting brass = 100%
Shear Modulus 8300 ksi(C71500 Annealed)
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000374 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.00 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 204 BTU-in/hr-ft²-°F
 29.2 W/m-K
@Temperature 100 °C
Mill Annealed (C71500)
 34.1 W/m-K
@Temperature 200 °C
Mill Annealed (C71500)
 38.6 W/m-K
@Temperature 300 °C
Mill Annealed (C71500)
 43.1 W/m-K
@Temperature 400 °C
Mill Annealed (C71500)
 48.1 W/m-K
@Temperature 500 °C
Mill Annealed (C71500)
 53.1 W/m-K
@Temperature 600.0 °C
Mill Annealed (C71500)
 58.1 W/m-K
@Temperature 700.0 °C
Mill Annealed (C71500)
Melting Point 2140 - 2260 °F
Solidus 2140 °F
Liquidus 2260 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 62.15 - 67.8 %As Remainder
Iron, Fe 1.7 - 2.3 %
Lead, Pb <= 0.050 %
Manganese, Mn 1.5 - 2.5 %
Nickel, Ni 29 - 32 %
Zinc, Zn <= 1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Copper nickel 30%, UNS C71500
Copper nickel 20%, UNS C71000
Copper nickel 10%, UNS C70600
California Fine Wire Nickel Alloy 180 Copper Nickel Resistance Wire
Carlson 70 30 Cu Ni Copper-Nickel Alloy

MC71640b1 / 11756

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.